Cold spray is a solid-state additive manufacturing process that has been increasingly used for restoration of damaged parts. Due to the nature of powder solid-state bonding, cold spray coatings usually possess pores in the microstructures. Heat treatment has been widely used as a post-processing method to reduce the porosity of cold sprayed coatings. However, it usually requires the whole component to be treated in the furnace and typically takes a few hours to finish the treatment. This study aims to develop a localized and rapid post-processing method for cold sprayed coatings. Multi-layer cold sprayed coatings of CoNiCrAlY on an Inconel 718 substrate were produced. Then the coatings were heat treated at 800 °C, 900 °C, 1000 °C and 1100 °C by rapid induction heating. The porosity level of the coatings reduced significantly after induction heating for a short period of merely 10 min. This is attributed to the preferential Joule heating at pore regions, which results in pore closures within the coatings. The potential application of induction heating as a rapid post-processing method for cold spray coatings has been demonstrated in this work.
Vacuum furnace has been used for brazing repair of aerospace components, but it is a slow process which typically takes a few hours. The prolonged heating and cooling cycles could cause some adverse effects on the components such as excessive grain growth. A rapid brazing technique using induction coil was studied to evaluate its suitability for localized repair. Induction brazing of Inconel 718 was carried out using AMS 4777 brazing paste at different temperatures (950 °C, 1050 °C and 1150 °C ) for various durations (2 min, 10 min and 20 min). Microstructure and microhardness were evaluated. The experimental results show that brazing at 1050 °C leads to desirable microstructures in a short period of merely 2 min. The study demonstrates the potential application of induction brazing for rapid localized aerospace repair.
Joining metals and ceramics plays a crucial role in many engineering applications. The current research aims to develop a simple and convenient approach for dissimilar material joining between SiC and Al alloys. In this work, Al alloys with Si contents varying from 7 wt.% to 50 wt.% were bonded with SiC at a high temperature of 1100 °C by a pressure-less bonding process in a vacuum furnace, and shear tests were carried out to study the bonding strength. When using low-Si Al alloys to bond with SiC, the bonding strength was very low. The bonding strength of Al/SiC joints increased significantly through the use of high-Si Al alloys with 30 wt.% and 50 wt.% Si. The shear strength achieved (28.8 MPa) is far higher than those reported previously. The remarkable improvement in bonding strength is attributed to the suppression of brittle interfacial products and reduced thermal stresses. This research provides a new strategy for joining between SiC and a wide range of Al alloys through the use of high-Si Al alloys as the interlayers.
1. Pursuing high strength while maintaining good ductility is challenging for metallic engineering materials due to strength-ductility trade-off [1]. Heterostructured materials (HMs) provide a solu...