Considerable research has been carried out to study the laser welding of magnesium alloys. However, the studies are mainly devoted to butt welding, and there has been limited information in the published literature concerning the bead-on-plate laser welding of AZ91D, even though bead-on-plate welding is required for the repair of cast AZ91D parts with surface defects. In the present investigation, surface cracking of the weld metal was observed when an AZ91D magnesium alloy was bead-on-plate welded using the laser welding method. This paper presents the experimental results and analyses to show that the cracking is “solidification cracking” initiated from the weld surface under high thermal stresses. This is in contrast to the “liquation cracking” observed in heat affected zones in tungsten inert gas welding of the same magnesium alloy. Laser power was found to be one of the main factors affecting the distance of the crack propagation. The higher laser power resulted in longer crack propagation distance into the weld metal. It is demonstrated that hot cracking could be avoided by lowering the laser power and welding speed.
Cold spray is a solid-state additive manufacturing process that has been increasingly used for restoration of damaged parts. Due to the nature of powder solid-state bonding, cold spray coatings usually possess pores in the microstructures. Heat treatment has been widely used as a post-processing method to reduce the porosity of cold sprayed coatings. However, it usually requires the whole component to be treated in the furnace and typically takes a few hours to finish the treatment. This study aims to develop a localized and rapid post-processing method for cold sprayed coatings. Multi-layer cold sprayed coatings of CoNiCrAlY on an Inconel 718 substrate were produced. Then the coatings were heat treated at 800 °C, 900 °C, 1000 °C and 1100 °C by rapid induction heating. The porosity level of the coatings reduced significantly after induction heating for a short period of merely 10 min. This is attributed to the preferential Joule heating at pore regions, which results in pore closures within the coatings. The potential application of induction heating as a rapid post-processing method for cold spray coatings has been demonstrated in this work.
Decarburization deteriorates the surface mechanical properties of steel. It refers to the loss of carbon from steel’s surface when exposed to an open-air environment in elevated-temperature conditions. Despite the short interaction time and fast thermal cycle of the laser surface-hardening process, decarburization may still occur. This paper investigates if decarburization occurs during the laser surface hardening of AISI 420 martensitic stainless steel. For comparison, surface-hardening results and decarburizations in a conventional air furnace-heated hardening process (water-quenched and air-cooled) of the same steel material were also investigated. Decarburization seems to have occurred in the laser surface hardening of AISI 420SS. However, the decarburization might not be significant, as the hardness of the steel’s surface was increased more than three times to 675 HV during the laser surface hardening, and the hardness drop due to decarburization was estimated to be only 3% with the decarburization depth of 40 μm. Simulations using ThermoCalc software to get the carbon concentration profiles along the depth for both laser-hardened and furnace-heated samples were also investigated.
Decarburization is an unwanted carbon-loss phenomenon on the surfaces of a material when they are exposed to oxidizing environments at elevated temperatures. Decarburization of steels after heat treatment has been widely studied and reported. However, up to now, there has not been any systematic study on the decarburization of additively manufactured parts. Wire-arc additive manufacturing (WAAM) is an efficient additive manufacturing process for producing large engineering parts. As the parts produced by WAAM are usually large in size, the use of a vacuum environment to prevent decarburization is not always feasible. Therefore, there is a need to study the decarburization of WAAM-produced parts, especially after the heat treatment processes. This study investigated the decarburization of a WAAM-produced ER70S-6 steel using both the as-printed material and samples heat-treated at different temperatures (800 °C, 850 °C, 900 °C, and 950 °C) for different durations (30 min, 60 min, and 90 min). Furthermore, numerical simulation was carried out using Thermo-Calc computational software to predict the carbon concentration profiles of the steel during the heat treatment processes. Decarburization was found to occur not only in the heat-treated samples but also on the surfaces of the as-printed parts (despite the use of Ar for shielding). The decarburization depth was found to increase with an increase in heat treatment temperature or duration. The part heat-treated at the lowest temperature of 800 °C for merely 30 min was observed to have a large decarburization depth of about 200 μm. For the same heating duration of 30 min, an increase in temperature of 150 °C to 950 °C increased the decarburization depth drastically by 150% to 500 μm. This study serves well to demonstrate the need for further study to control or minimize decarburization for the purpose of ensuring the quality and reliability of additively manufactured engineering components.
Vacuum furnace has been used for brazing repair of aerospace components, but it is a slow process which typically takes a few hours. The prolonged heating and cooling cycles could cause some adverse effects on the components such as excessive grain growth. A rapid brazing technique using induction coil was studied to evaluate its suitability for localized repair. Induction brazing of Inconel 718 was carried out using AMS 4777 brazing paste at different temperatures (950 °C, 1050 °C and 1150 °C ) for various durations (2 min, 10 min and 20 min). Microstructure and microhardness were evaluated. The experimental results show that brazing at 1050 °C leads to desirable microstructures in a short period of merely 2 min. The study demonstrates the potential application of induction brazing for rapid localized aerospace repair.