Crystalline nanocellulose was prepared from Semantan bamboo (Gigantochloa scortechinii) via acid hydrolysis and was used to synthesize a nanocomposite of polyaniline/crystalline nanocellulose (PANi/CNC) via in situ oxidative polymerization of aniline in the presence of crystalline nanocellulose. The electrochemical properties of the nanocomposite were studied using a modified PANi/CNC electrode via cyclic voltammetry, and higher current response was observed for the PANi/CNC-modified electrode compared to that for the modified electrode with PANi. The results obtained from EIS displayed lower value of Rct for the PANi/CNC-modified electrode, indicating that the incorporation of CNC into the PANi structure could enhance the electron transfer rate. The characteristic peaks of PANi and CNC were observed in the FTIR spectra of the nanocomposite, indicating the incorporation of CNC inside the nanocomposite structure. Moreover, in the XRD diffractogram, lower crystallinity was observed at the 2 theta values of 22.6 and 16.1 for PANi/CNC compared to that for pure CNC. The FESEM images showed high porosity of the nanostructure with no phase separation, revealing the homogenous polymerization of the monomer on the surface of the crystalline cellulose. Aggregation of PANi particles was observed with the increasing aniline concentration.
Effects of Alkaline Sulfite Anthraquinone and Methanol Pulping Conditions on the Mechanical and Optical Paper Properties of Bamboo (Gigantochloa scortechinii)
23 October 2017 in European Journal of Wood and Wood Products
This chapter explores the characteristic potentials of alkaline sulfite anthraquinone and methanol (ASAM) pulping of bamboo culms (Gigantochloa scortechinii) in the industrial production of pulp and paper for packaging. The biometric characterization results of the bamboo culms show that bamboo has fiber length of 1980–4000 μm, Runkel ratio of 0.86, and flexibility ratio of 50.19, while the chemical compositions of the bamboo contain 47.67% cellulose, 68.33% holocellulose, 26% lignin, and 3.69% solvent extractive, which give good paper quality fiber and also falls within the range of wood from softwoods species. The study revealed that the optimum ASAM pulping parameters was at 16% NaOH and 90 min cooking time, resulting in Kappa number of 14.17 and pulp yield of 49.06%, while the paper tensile index of 20.86 Nm/g, tear index of 22.64 mN.m2/g, and brightness of 39.32% were obtained. The biometric and chemical characterizations of the ASAM pulped bamboo have shown that ASAM pulped bamboo produces high-quality pulp and paper suitable for packaging and printing paper. Hence, the use of bamboo materials can reduce the burden on the forest, due to the increasing demand for paper and paper products, while supporting the natural biodiversity.