Carbon powders exhibit electrical conductivity that causes the powders to agglomerate due to the applied electrostatic forces and discharges capacitance when used for surface treatments with plasma sources. To avoid this obstacle, a non-direct method is used with active gas that is generated through plasma. This active gas is in contact with the carbon powder so that the hydrophilic characteristics are formed. It is the carboxyl COO− functional group that causes hydrophilic improvement and it is shown to increase in the carbon surface after soft oxidation. The wettability of carbon powder gradually improves with more plasma treatment time. This is shown through a simple water dispersion test. Eventually, the dispersed aqueous solution gradually separates the powder, which either floats or sinks. The sample treated for 60 min is shown to continuously sustain dispersibility in water over a long period of time.
18 January 2019 in IEEE Transactions on Plasma Science
The surface of 180-μm polyethylene (PE) and 200-nm polytetrafluoroethylene (PTFE) powders are hydrophilized by using surface dielectric barrier discharge (sDBD) applied to a batch of 20 g for both cases. On the sDBD electrode, charged particles by plasma generation are able to diffuse onto the power surface through small voids. In order to know the level of hydrophilic treatment on the powder, absorption tests by using droplet was carried out. This principle is based on the fact that the inner gap between powders are small enough that a liquid with a certain surface tension is absorbed or formed on powder layer when dropped on the powder surface. The minimum isopropyl alcohol (IPA) concentration absorbed into the powder was measured by an aqueous solution with a mixture of IPA and D.I water. By lowering the IPA concentration, improvements in the hydrophilicity were obtained. The concentration of IPA before treatment of PE powder was 15% and decreased to 3% after treatment. In the case of PTFE, IPA concentration decreased slightly from 39% to 30% after the treatment. Also, the surface treated PE and PTFE displays a significant difference in the degree of dispersion in water and n-methyl pyrollidone solvent. In the field-emission scanning electron microscope analysis, the morphology of the treated surface was clean. From composition of the surface by X-ray photoelectron spectroscopy, when the untreated sample is 100% C-H, the plasma treated PE shows 82.48% C-H, and 17.52% C-O. A partial change in the C-F bond is shown for PTFE.
SiC wafers were etched using a filament plasma of He:NF3:O2 (helium:nitrogen trifluoride:oxygen) mixed gas at atmospheric pressure. When 0.5–2 sccm of NF3 was mixed to 2 slm of He filament plasma, the etch depth and etch rate increased, but there was little change in the etch width as the NF3 mixing amount increased. The increment of the NF3 mixing also suppressed the surface roughening of plasma etching. The addition of O2 to the He-NF3 filament plasma slightly increased the SiC wafer etch rate. When the NF3 mixing amount was 2 sccm, the roughness of the etched surface increased sharply by O2 addition. On the contrary, the NF3 mixing amount was 1 sccm; the addition of O2 reduced the roughness more than that of the pristine. The roughness of the pristine SiC wafer specimens is in the range of Ra 0.7–0.8 nm. After 30 min of etching on a 6 mm by 6 mm square area, the roughness of the etched surface reduced to Ra 0.587 nm, while the etch rate was 2.74 μm/h with a He:NF3:O2 of 2:1:3 (slm:sccm:sccm) filament plasma and 3 mm/s speed of raster scan etch of the optimized roughening suppression etching recipe.