Carbon powders exhibit electrical conductivity that causes the powders to agglomerate due to the applied electrostatic forces and discharges capacitance when used for surface treatments with plasma sources. To avoid this obstacle, a non-direct method is used with active gas that is generated through plasma. This active gas is in contact with the carbon powder so that the hydrophilic characteristics are formed. It is the carboxyl COO− functional group that causes hydrophilic improvement and it is shown to increase in the carbon surface after soft oxidation. The wettability of carbon powder gradually improves with more plasma treatment time. This is shown through a simple water dispersion test. Eventually, the dispersed aqueous solution gradually separates the powder, which either floats or sinks. The sample treated for 60 min is shown to continuously sustain dispersibility in water over a long period of time.
SiC wafers were etched using a filament plasma of He:NF3:O2 (helium:nitrogen trifluoride:oxygen) mixed gas at atmospheric pressure. When 0.5–2 sccm of NF3 was mixed to 2 slm of He filament plasma, the etch depth and etch rate increased, but there was little change in the etch width as the NF3 mixing amount increased. The increment of the NF3 mixing also suppressed the surface roughening of plasma etching. The addition of O2 to the He-NF3 filament plasma slightly increased the SiC wafer etch rate. When the NF3 mixing amount was 2 sccm, the roughness of the etched surface increased sharply by O2 addition. On the contrary, the NF3 mixing amount was 1 sccm; the addition of O2 reduced the roughness more than that of the pristine. The roughness of the pristine SiC wafer specimens is in the range of Ra 0.7–0.8 nm. After 30 min of etching on a 6 mm by 6 mm square area, the roughness of the etched surface reduced to Ra 0.587 nm, while the etch rate was 2.74 μm/h with a He:NF3:O2 of 2:1:3 (slm:sccm:sccm) filament plasma and 3 mm/s speed of raster scan etch of the optimized roughening suppression etching recipe.