Graphene nanosheets (GNS) were prepared from graphitic oxide (GO) in two different ways: (a) thermal exfoliation at different temperatures; and (b) wet chemistry, using aqueous N2H4 and KBH4 as reducing agents. Irrespective of the synthetic method used, the materials exhibited a high irreversible capacity and strong polarization in their charge curves, when used in a Li-ion battery. The GNS synthesized with N2H4 exhibited the best performance. Thus, at 149 mA g−1 the average specific capacity delivered was ca. 600 mA h g−1 after 100 cycles. On the other hand, the worst performance, irrespective of rate, was that of GNS synthesized with KBH4 and the thermal GNS obtained at 800 °C. The physical and chemical analyses allowed various parameters to be derived for correlation with the electrochemical properties. Unfortunately, no clear-cut correlation was apparent. A comparison with reported data revealed that no correlation appears to exist with physical and chemical properties that allows a simple strategy for tailoring an effective graphene anode to be designed.
Graphene nanosheets (GNS) are synthesized from untreated natural graphite (NG) for use as electroactive materials in Li-ion batteries (LIBs), which avoids the pollution-generating steps of purifying graphite. Through a modified Hummer method and subsequent thermal exfoliation, graphitic oxide and graphene were synthesized and characterized structurally, morphologically and chemically. Untreated natural graphite samples contain 45–50% carbon by weight; the rest is composed of different elements such as aluminium, calcium, iron, silicon and oxygen, which are present as calcium carbonate and silicates of aluminium and iron. Our results confirm that in the GO and GNS synthesized, calcium is removed due to oxidation, though other impurities are maintained because they are not affected by the synthesis. Despite the remaining mineral phases, the energy storage capacity of GNS electrodes is very promising. In addition, an electrochemical comparison between GNS and NG demonstrated that the specific capacity in GNS is higher during the whole cycling process, 770 mA·g−1 at 100th cycle, which is twice that of graphite.