Fiber waviness defects are found in the inner surface of the hat-shaped stringers manufactured by a process system. In order to establish the acceptance criterion for the stringers with the fiber waviness defects, experimental testing and numerical simulation were carried out in this study. Specially induced fiber waviness defects of four pre-defined severity levels were manufactured and tested. A maximum of a 58.1% drop in compressive failure load is observed for the most severe level in the experimental results. A finite element model with progressive damage method and cohesive zone technique was developed to simulate the failure process and the impact of fiber waviness defects. The numerical simulation results of compressive failure load have a good agreement with experimental results qualitatively and quantitatively. In addition, two simple parameters, i.e., aspect ratio A/H and the number of plies with fiber waviness, are proposed to characterize the influence of the fiber waviness on the compressive failure load for the purpose of fast engineering quality checks.
The tack of prepreg is a key factor affecting the automatic tape laying process. During the manufacturing process of large composite parts, prepreg material may be stored at room temperature for several days, resulting in a decrease in its tack. In this study, a new tack test tool was designed, and the decay rate of prepreg tack at different temperatures was tested. We proposed a prepreg tack decay model, which assumes that the main factor in tack decay is the reduction in resin chain activity during storage. The maximum deviation between the model calculation results and the experimental results of the tack decay rate is 9.7%. This study also proposed a new statistical unit for prepreg tack, which can establish the relationship between the tack of prepreg and its remaining storage time and reduce prepreg management costs.
Tack is one of the most important factors affecting the operability of prepregs, but it is still very difficult to obtain the change of prepreg tack with time at different temperatures. In this paper, a newly designed T-peel device is used to test the tack decay rate of prepregs at different temperatures. The obtained decay rate deviates less than 8.9% from the manufacturer's data. The maximum deviation of the ratio of tack decay speeds calculated by the Arrhenius equation from the experiments is not higher than -9.7%. It is proved that the present method can obtain the decay rate of tack of prepregs at different temperatures. This method is also applicable to the other two types of prepregs. The article proposes the handling life unit, an operational life measurement unit for prepregs, and establishes that the relationship between tack and remaining shelf life reduces prepreg management costs.