Stripped-back representative VCSEL devices with a simple fabrication process that very closely approaches the performance of standard BCB-planarised devices have been produced. These VCSEL Quick Fabrication (VQF) devices achieve threshold currents only 0.3 mA higher than that of a standard device produced from the same material. The predictability of standard performance from VQF performance is also robustly assessed in terms of temperature effects to account for the observed disparities. These VQF devices are then processed across a 6-inch (152 mm) wafer and the resulting device-level characteristics are mapped. From this, it is apparent that there is an approximately radial decrease in oxide aperture diameter from centre to edge, found to be driven by the strain-induced wafer bow. After corrections, a residual spatial variation across the wafer remains, which, in conjunction with temperature dependent measurements, is shown to be a result of epi-material variation. By observation at 50 °C, that is, at a temperature closely resembling that of intended application, the residual centre-to-edge variation in threshold current density is found to be only 0.2 kA/cm 2 , compared to 1.3 kA/cm 2 when observing the room temperature variation of devices of nominally equivalent active volumes.
13 March 2023 in Journal of Physics D: Applied Physics
Vertical cavity surface emitting laser (VCSEL) devices and arrays are increasingly important in meeting the demands of today’s wireless communication and sensing systems. Understanding the origin of non-uniform wet thermal oxidation across large-area VCSEL wafers is a crucial issue to ensure highly reliable, volume-manufactured oxide-confined VCSEL devices. As VCSEL wafer diameters approach 200 mm, germanium (Ge) is emerging as an alternative substrate solution. To this end, we investigate the uniformity of 940 nm-emitting VCSEL performance across 150 mm diameter GaAs- and Ge-substrates, comparing the oxidation method in each case. Nominally identical epitaxial structures are used to evaluate the strain induced wafer bow for each substrate type with Ge exhibiting a reduction of over 100 μm in the peak-to-valley distortion when compared with GaAs. This wafer bow is found to be the principal cause of centre-to-edge oxidation non-uniformity when utilising a conduction-heated chuck furnace, in comparison to a convection-heated tube furnace. Using on-wafer testing of threshold current, differential resistance, and emission wavelength, device performance is demonstrated for the first time across a 150 mm Ge wafer, and is shown to be comparable to performance on GaAs substrates, when the effects of oxidation uniformity are removed. These results provide evidence that there is a realistic path to manufacturing high yield VCSELs, over wafer diameters approaching those used in Si-photonics, via Ge substrates.
31 January 2023 in Journal of Physics D: Applied Physics
We report direct measurements of the optical gain on vertical-cavity surface-emitting laser (VCSEL) material using a stripe-length method featuring segmented contacts. We utilise the similarity of the in-plane transverse electric (TE) polarised matrix element and that of the VCSEL lasing mode and a simple method to reduce round trip effects. The confinement factor is determined from cold-cavity simulations of the in-plane TE polarised slab waveguide mode and used to convert the measured in-plane modal gain into the vertical-cavity modal gain, as required for the VCSEL structure. This gives a threshold material gain of 1440 ± 140 cm−1 at 30 °C for this structure. A comparison with the threshold material gain values determined from the lasing condition, where internal optical losses due to doping induced absorption is included using parameters taken from the literature, indicates the presence of an additional source of optical loss in the experiment which increases the threshold material gain by ∼450 cm−1. A best fit is obtained by increasing the optical loss in the n-DBR (distributed Bragg reflectors) layers to 40 cm−1, which is consistent with previous work on additional scattering losses due to interface roughening in the n-DBR layers. To further demonstrate the utility of this method for rapid optimisation, the gain-peak wavelength is measured directly, and its temperature dependence is compared to the lasing wavelength.
This work presents an approach to assess the quality of etched laser facets, considering factors such as roughness, inclination, and non-uniform light emission. Broad area InP lasers, using plasma etched facets, operating at 1550 nm are manufactured with varying facet quality on five 100 mm wafers. Comparison of the threshold current density of lasers of different length was used to derive relative facet reflectivity and demonstrated the relationship between the reflectivity and the optical mode weighted facet roughness and facet inclination.
VCSEL thermal resistances are determined from power-current-voltage-wavelength measurements performed on nominally identical epitaxial structures grown on Ge and GaAs substrates. We show that the effective thermal conductivity of the VCSEL is increased when grown on Ge substrates.
A systematic analysis of the performance of VCSELs, fabricated with a decreasing number of structural elements, is used to assess the complexity of fabrication (and therefore time) required to obtain sufficient information on epitaxial wafer suitability. Initially, sub-mA threshold current VCSEL devices are produced on AlGaAs-based material, designed for 940 nm emission, using processing methods widely employed in industry. From there, stripped-back Quick Fabrication (QF) devices, based on a bridge-mesa design, are fabricated and this negates the need for benzocyclcobutane (BCB) planarisation. Devices are produced with three variations on the QF design, to characterise the impact on laser performance from removing time-consuming process steps, including wet thermal oxidation and mechanical lapping used to reduce substrate thickness. An increase in threshold current of 1.5 mA for oxidised QF devices, relative to the standard VCSELs, and a further increase of 1.9 mA for unoxidised QF devices are observed, which is a result of leakage current. The tuning of the emission wavelength with current increases by 0.1 nm/mA for a VCSEL with a 16 μm diameter mesa when the substrate is unlapped, which is ascribed to the increased thermal resistance. Generally, relative to the standard VCSELs, the QF methods employed do not significantly impact the threshold lasing wavelength and the differences in mean wavelengths of the device types that are observed are attributed to variation in cavity resonance with spatial position across the wafer, as determined by photovoltage spectroscopy measurements.