The growing demand for composite materials with improved properties is attracting a lot of attention from industries such as automotive, aerospace, military, aviation, and other manufacturing. Aluminium metal matrix composites (AMMCs), with various reinforcements such as continuous/discontinuous fibers, whiskers, and particulates, have captured the attention due to their superior tribological, mechanical, and microstructural characteristics as compared to bare Al alloy. AMMCs have undergone extensive research and development with different reinforcements in order to obtain the materials with the desired characteristics. In this paper, we present a review on AMMCs produced through stir casting routes. This review focuses on the following aspects: (i) different reinforcing materials in AMMCs; (ii) microstructural study of reinforced metal matrix composites (MMCs) through stir casting. Both reinforcing micro- and nanoparticles are focused. Micro- and nanoreinforced AMMCs have the attractive properties of combination such asthe low-weight-to-high-strength rati and, low density; (iii) various tribological and mechanical properties with the consideration of different input parameters; (iv) outlook and perspective.
5 December 2015 in Korean Journal of Metals and Materials
AlCrSiN film with a composition of 29.1Al-17.1Cr-2.1Si-51.7N in at. % was deposited on a steel substrate by cathodic arc ion plating at a thickness of 1.8 μm. It consisted of nanocrystalline hcp-AlN and fcc-CrN, where a small amount of Si was dissolved. Corrosion tests were carried out at 800 °C for 5–200 h in Ar-1%SO2 gas. The major corrosion reaction was oxidation owing to the high oxygen affinity of Al and Cr in the film. The formed oxide scale consisted primarily of (Al,Cr)2O3, within which Fe, Si, and S were dissolved. Even after corrosion for 200 h, the thickness of the scale was about 0.7–1.2 μm, indicating that the film had good corrosion resistance in the SO2-containing atmosphere.
1 November 2016 in Journal of Nanoscience and Nanotechnology
The Ni-based superalloy, Inconel 738LC, was corroded between 800 and 1000 °C for up to 100 h in the Ar/0.2%SO2 gas. The formed scales were susceptible to breakage and spallation, due partly to the incorporation of sulfur. They consisted primarily of Cr2O3, along with some TiO2 and NiO. Preferential oxidation of Cr to Cr2O3 led to the Cr depletion in the Al2O3-rich internal oxidation zone, where Ni, Co, W, and Ta tended to accumulate as corrosion progressed.
30 April 2016 in Journal of the Korean institute of surface engineering