Pelvic organ prolapse (POP) is a multifactorial connective tissue disorder caused by damage to the supportive structures of the pelvic floor, leading to the descent of pelvic organs in the vagina. In women with POP, fibroblast function is disturbed or altered, which causes impaired collagen metabolism that affects the mechanical properties of the tissue. Ideal surgical repair, either native tissue repair or POP surgery using an implant, aims to create a functional pelvic floor that is load-bearing, activating fibroblasts to regulate collagen metabolism without creating fibrotic tissue. Fibroblast function plays a crucial role in the pathophysiology of POP by directly affecting the connective tissue quality. On the other hand, fibroblasts determine the success of the POP treatment, as the fibroblast-to-(myo)fibroblast transition is the key event during wound healing and tissue repair. In this review, we aim to resolve the question of “cause and result” for the fibroblasts in the development and treatment of POP. This review may contribute to preventing the development and progress of anatomical abnormalities involved in POP and to optimizing surgical outcomes.
Electrochemical impedance spectroscopy (EIS) and spectroscopy was applied to investigate the surface activation of carboxyl group (–COOH) containing nanofibers by the reaction of 1-ethyl-3-(dimethyl-aminopropyl) carbodiimide hydrochloride (EDC)/N-hydroxyl succinimide (NHS) in different concentrations. Poly(!-caprolactone)/poly(m-anthranilic acid) (PCL/P3ANA) nanofibers were fabricated by electrospinning and were activated with 5/0.5, 0.5/5, 5/5 and 50/50 mM of EDC/NHS. The surface activation was investigated by Attenuated Total Reflectance Fourier transform infrared spectroscopy (FTIR-ATR) and activation yield was estimated. Albumin was immobilized after surface activation and the amount of covalently immobilized protein was determined by bicinchoninic acid (BCA) assay. Morphology and composition of albumin immobilized nanofibers were characterized by Scanning Electron Microscopy/Energy-Dispersive X-ray Spectroscopy (SEM/EDX) and Atomic force microscope (AFM). EIS measurements indicated that nanofibers become resistant after albumin immobilization. The obtained data revealed that the highest amount of albumin bound to nanofibers activated with 50/50 mM of EDC/NHS which was found to be the optimum concentration for the activation of PCL/P3ANA nanofibers
22 June 2016 in International Journal of Polymeric Materials and Polymeric Biomaterials
RGD functionalized nanofibers of poly(ε-caprolactone)/poly(m-anthranilic acid) (PCL/P3ANA) were fabricated to address the mechanical, structural and functional requirements of bone tissue engineering. Nanofibers containing the highest amount of P3ANA with more carboxyl groups for functionalization have exhibited higher surface area and better mechanical properties. FTIR-ATR and UV-visible measurements evidenced the covalent RGD immobilization. After RGD peptide immobilization, the surface properties of nanofibers changed as evidenced by contact angle and electrochemical impedance spectroscopy (EIS). The effects of RGD functionalized nanofibers (PCL/P3ANA-RGD) on Saos-2 cell attachment, proliferation, and osteogenic activity were investigated. PCL/P3ANA-RGD nanofibers favored cell attachment, proliferation, and osteogenic activity. GRAPHICAL ABSTRACT
1 January 2018 in Sensors and Actuators B: Chemical
Objective: To evaluate the host‐ and biomechanical response to a fully absorbable poly‐4‐hydroxybutyrate (P4HB) scaffold in comparison with the response to polypropylene (PP) mesh.Design: In vivo animal experiment.Setting: KU Leuven Center for Surgical Technologies.Population: Fourteen parous female Mule sheep.Methods: P4HB scaffolds were surgically implanted in the posterior vaginal wall of sheep. The comparative PP mesh data were obtained from an identical study protocol performed previously.Main outcome measures: Gross necropsy, host response and biomechanical evaluation of explants, and the in vivo P4HB scaffold degradation were evaluated at 60‐ and 180‐days post‐implantation. Data are reported as mean ± standard deviation (SD) or standard error of the mean (SEM).Results: Gross necropsy revealed no implant‐related adverse events using P4HB scaffolds. The tensile stiffness of the P4HB explants increased at 180‐days (12.498 ± 2.66 N/mm SEM [p =0.019]) as compared to 60‐days (4.585 ± 1.57 N/mm) post‐implantation, while P4HB degraded gradually. P4HB scaffolds exhibited excellent tissue integration with dense connective tissue and a moderate initial host response. P4HB scaffolds induced a significantly higher M2/M1 ratio (1.70 ± 0.67 SD, score 0–4), as compared to PP mesh(0.99 ± 0.78 SD, score 0–4) at 180‐days.Conclusions: P4HB scaffold facilitated a gradual load transfer to vaginal tissue over time. The fully absorbable P4HB scaffold, in comparison to PP mesh, has a favorable host response with comparable load‐bearing capacity. If these results are also observed at longer follow‐up in‐vivo, a clinical study using P4HB for vaginal POP surgery may be warranted to demonstrate efficacy.Tweetable Degradable vaginal P4HB implant might be a solution for treatment of POP.