Chengde chromium-bearing vanadium–titanium magnetite (CCVTM) has been used as an important mineral resource in sinter making. The MgO content of this sinter can be enhanced by adding dolomite, which improved operation of the blast furnace. The effects of MgO in the form of dolomite on metallurgical properties, microstructure and mineral compositions of CCVTM sinter were studied by a sinter pot test, X-Ray Diffraction (XRD), Scanning Electron Microscope (SEM), and mineral phase microanalysis. The results were as follows: The flame front speed and sinter coefficient decreased with an increase in MgO content from 2.66 to 3.86% by adding dolomite. With an increase in MgO content from 2.66 to 3.86%, the flame front speed, sintering utilization factor, and the value of RI decreased, while RDI and the softening–melting properties improved. In addition, the value of sinter strength (TI) reached a maximum value at MgO = 3.56%. In addition, an increase in the abundance of magnetite, magnesium ferrite, and silicate phase, as well as a decrease in hematite, was found with an increase in MgO content. We concluded that the most appropriate MgO content in the sinter is 3.56%.
The sinter process of iron ore with biomass carbon instead of coke breeze as fuel was investigated via thermodynamic analysis in this paper through a comparison of sinter composition indexes, metallurgical properties, and pollutant emissions. Straw charcoal was used in this paper, and its replacement does not adversely affect the composition index of iron ore, namely Fe, FeO, basicity, S, nor the metallurgical properties, namely reduction degradation index and reduction index. However, the replacement has a great effect on the emissions of pollutant gases, including SO2, NOx, CO, and CO2. The thermodynamic analysis result shows that emissions of pollutant gases produced in the sinter process significantly decrease by using straw charcoal instead of coke breeze in sinter. The sintering maximum temperature has a great influence on sintering technical indicators. The best sintering maximum temperature is between 1300 and 1400 °C, where sinter ore with high quality can be obtained.
The influence of fuel level on Russian vanadiferous titanomagnetite sinter properties, productivity, and mineralogy are researched by sintering pot testing, metallographic microscopy, scanning electron microscopy analysis, and energy dispersive spectrometer (SEM-EDS) analysis. A comprehensive index is evaluated in conjunction with the same indexes and significance coefficient as that in the Panzhihua Iron and Steel Group. Results show that with the increasing fuel level from 3.5% to 6.0%, flame front speed, yield, tumbling test index (TI), and productivity, all first increase and then decrease. The low temperature reduction degradation index (RDI+3.15) and softening zone (ΔT) gradually increase while the RI and starting temperature of softening (T10), and ending temperature of softening (T40) decrease with increasing fuel levels from 3.5% to 6.0%. With the increase of fuel level from 3.5% to 6.0%, the content of FeO, SiO2, and MgO increase, while TiO2 shows a decrease. For the same increase in fuel level, the number of pores and calcium ferrite and hematite decrease but the silicate increases. In addition, in the fuel level range of 3.5% to 5.5%, magnetite correspondingly increases but then shows a drop after 5.5%. Moreover, when the fuel level increases to greater than 5.0%, FeOx and fayalite quickly increase and a small amount of metallic iron appears under the fuel level of 6.0%. Overall, the optimal fuel level under current production conditions and indicator selection is 4.0%.
The double-effect Ni-based catalysts, modified with Ce, Mg, and Fe and synthesized by the coprecipitation method, were applied into the enhanced steam reforming process of real tar. The effects of the catalysts with different doping mass proportions (3, 6, 9, and 12%) of Ce, Mg, and Fe on the H2 yield, and H2 and CO2 concentrations were studied. The results revealed that the tar reforming efficiency was improved with appropriate proportions of the additives added. The Ce- or Mg-doped catalyst could change the distribution or morphology of the active component Ni. The modified catalyst with 6% Ce or 3% Mg doping showed the best catalytic activity in the reforming experiment, with the H2 yield reaching 86.84% or 85.22%, respectively. The Fe-doped catalyst could form an Ni–Fe alloy and improve the stability of the catalyst, and the better catalytic activity can be obtained at 9 and 12% Fe doping, with the H2 yield reaching 85.54 and 85.80%, respectively.