Ceramifiable silicone rubber composites play important roles in the field of thermal protection systems (TPS) for rocket motor cases due to their advantages. Ceramifiable silicone rubber composites filled with different contents of ZrSi2 were prepared in this paper. The fffects of ZrSi2 on the vulcanization, mechanical and ablation resistance properties of the composites were also investigated. The results showed that the introduction of ZrSi2 decreased the vulcanization time of silicone rubber. FTIR spectra showed that ZrSi2 did not participate in reactions of the functional groups of silicone rubber. With the increasing content of ZrSi2, the tensile strength increased first and then decreased. The elongation at break decreased and the permanent deformation increased gradually. The thermal conductivity of the composite increased from 0.553 W/(m·K) to 0.694 W/(m·K) as the content of the ZrSi2 increased from 0 to 40 phr. In addition, the thermal conductivity of the composite decreased with the increase of temperature. Moreover, thermal analysis showed that the addition of ZrSi2 increased the initial decomposition temperature of the composite, but had little effect on the peak decomposition temperature in nitrogen. However, the thermal decomposition temperature of the composite in air was lower than that in nitrogen. The addition of ZrSi2 decreased the linear and mass ablation rate, which improved the ablative resistance of the composite. With the ZrSi2 content of 30 phr, the linear and mass ablation rate were 0.041 mm/s and 0.029 g/s, decreasing by 57.5% and 46.3% compared with the composite without ZrSi2, respectively. Consequently, the ceramifiable silicone rubber composite filled with ZrSi2 is very promising for TPS.
The application of epoxy resins in high temperature and thermal protection fields is limited due to their low decomposition temperature and low carbon residual rate. In this paper, epoxy resin (EP)/quartz fiber (QF) ceramifiable composites were prepared using a prepreg-molding process. The thermal stability, phase change and mechanical properties after high-temperature static ablation and ceramization mechanism of EP/QF ceramifiable composites were investigated. The addition of glass frits and kaolinite ceramic filler dramatically increases the thermal stability of the composites, according to thermogravimetric (TG) studies. The composite has a maximum residual weight of 61.08%. The X-ray diffraction (XRD) results show that the mullite ceramic phase is generated, and a strong quartz diffraction peak appears at 1000 °C. The scanning electron microscope (SEM) and element distribution analyses reveal that the ceramic phase generated inside the material, when the temperature reaches 1000 °C, effectively fills the voids in composites. The composites have a bending strength of 175.37 MPa at room temperature and retain a maximum bending strength of 12.89 MPa after 1000 °C treatment.
Zirconia fibres have excellent high temperature ablation resistance and have been widely used in ablative materials. In this paper, zirconia fibre was used for reinforcing the ablative composite materials to study the influence of zirconia fibre had upon the mechanical properties and the high temperature ablation properties of such composites. The results showed that the bending strength of the material was also good and reached a maximum of 13.05 MPa. After sintering at 1400°C, the bending strength was also great which could reach 13.05 MPa. In addition, the corrosion resistance of the composites was excellent and the oxygen-acetylene line ablation rate was 0.03 mm s−1 when the fibre content was 30 wt-%.
Boron phenolic resin is widely used in the aerospace field because of its excellent thermal properties. In this article, nitrile rubber powder was added to phenolic resin to modify fiber-reinforced phenolic resin composites. The results showed that the tensile strength continued to decrease; the elongation ratio increased from 20.01% to 32.04%; and flexural strength and flexural modulus reached the highest values of 188 and 9,401 MPa, respectively. Thermal analysis showed that rubber had little effect on the heat resistance at low temperatures, especially below 350°C. Furthermore, the coefficient of thermal expansion of the composites increased from 8.9 × 10 −6 to 1.5 × 10 −5 K −1 , increasing by nearly 70%. The electron microscopy images showed a tortuous fracture path in modified composites, which indicated that rubber powder–modified phenolic composites had a ductile fracture.
25 February 2020 in Plastics, Rubber and Composites: Macromolecular Engineering
With the development of rocket and aerospace technology in recent decades, people have put forward higher requirements on the heat resistance and ablation performance of thermal protection materials. In this paper, zirconia fibre hybrid alumina fibre/boron phenolic (ZA/BPF) ceramifiable composites, based on ceramic fillers of MgO, Al2O3, SiC and mica-modified boron phenolic resin matrix, were prepared with different hybrid fibre contents (5, 10, 15, 20, 25, 30 wt-%) by hot compression moulding. The result shows that fibre contents have little effect on the ablation resistance of composite materials which all have a low linear ablation rate below 0. 01 mm s−1. When the fiber content is 25%, the ZA/BPF composite reaches the highest bending strength 48. 86 MPa and 15. 57 MPa before and after sintering respectively. It is showed by the SEM results that too high and too low fibre content would both lead to poor bonding between resin and fibre interfaces.