The properties of Te-doped and Te-Ni double-doped nanostructured skutterudites were evaluated by means of x-ray powder diffraction, and transport properties measured on the synthesized samples have been compared with ab initio theoretical modeling. Theoretical optimal dopant contents have been evaluated according to the maximum value of the power factor, calculating the electronic transport properties from the ab initio material band structure using semiclassical Boltzmann transport theory. The samples have been synthesized by chemical alloying with Te substitution for Sb up to and Ni substitution for Co up to . X-ray powder diffraction has been performed on all samples to reveal information about phase purity and Rietveld refinement was performed for the phase composition and cell parameter. The thermoelectric properties of the resulting consolidates were investigated in a temperature range from using various measurement facilities. A standardization and round robin program was started among the participating evaluation laboratories in order to ensure reliability of the data obtained. The significant reduction in thermal conductivity, when compared to highly annealed , could be proved which is caused by the nanostructuring, resulting in a high concentration of grain boundaries. A combination of substitution levels for Ni and Te has been found resulting in the largest value of 0.65 at among unfilled skutterudite materials.
β-Zn4Sb3 is reported to have poor thermal stability and there is a wide scatter in the thermoelectric figure of merit (ZT) measured by different groups. Here, we show that both these issues are related to the zinc concentration. Specimens of β-Zn4Sb3 having different carrier concentrations (n) have been prepared and thermoelectric property measurements carried out between room temperature and 525 K. The maximum ZT is found to vary between 0.4 and 0.85. The cause of the large variation in ZT is the strong dependence of the lattice thermal conductivity (κL) on n which make ZT sensitive to small changes in zinc concentrations. Based on analytical calculations, we show that by changing the zinc interstitial to the zinc lattice ratio, it is possible to achieve the experimental κL variation. Thermal cycling of the electrical conductivity (σ) has been performed and phase identification after each cycling is carried out from power x-ray data. Different trends are observed in the specimens depending on n with accelerated degradation occurring only in a certain range of n (∼1.2–2.5 × 1020 cm−3) corresponding to low zinc content in the matrix.
29 December 2009 in Journal of Electronic Materials
Thermoelectric generators are a reliable and environmentally friendly source of electrical energy. A crucial step for their development is the maximization of their efficiency. The efficiency of a TEG is inversely related to its electrical contact resistance, which it is therefore essential to minimize. In this paper, we investigate the contacting of an Al electrode on Mg2(Si,Sn) thermoelectric material and find that samples can show highly asymmetric electrical contact resistivities on both sides of a leg (e.g., 10 µΩ·cm2 and 200 µΩ·cm2). Differential contacting experiments allow one to identify the oxide layer on the Al foil as well as the dicing of the pellets into legs are identified as the main origins of this behavior. In order to avoid any oxidation of the foil, a thin layer of Zn is sputtered after etching the Al surface; this method proves itself effective in keeping the contact resistivities of both interfaces equally low (<10 µΩ·cm2) after dicing. A slight gradient is observed in the n-type leg’s Seebeck coefficient after the contacting with the Zn-coated electrode and the role of Zn in this change is confirmed by comparing the experimental results to hybrid-density functional calculations of Zn point defects.