A plasma treatment of polymeric materials has become one of the most important methods to enhance the surface wettability without affecting the bulk material features. Oxygen plasma treatment of polystyrene surfaces deposited on a QCM sensor was evaluated by relating the plasma parameters, surface roughness, and the wettability. The internal plasma parameters investigated in this work were the electron temperature (Te) and the electron density (ne). The oxygen plasma was generated using an RF power generator. The power was varied by applying a voltage from 60 volts to 100 volts. An Optical Emission Spectroscopy (OES) was used to determine the plasma species, the Te and the ne during the plasma oxygen process. The dominant species in the plasma was excited atomic oxygen or activated oxygen (OI) which was detected from the 774 nm and 842 nm emissions. The higher applied RF voltage resulted in the higher Te and n e. The effect of the T e and n e on the polystyrene surface was observed on the change of the surface roughness. The surface roughness significantly related to the surface wettability observed with a contact angle measurement. Furthermore, the plasma treatment greatly changed the surface from hydrophobic to hydrophilic via reactive processes by the excited atomic oxygen species. This was confirmed by the increase in C=C and C=O functional groups observed using a Fourier transform infrared (FTIR) spectroscopy. The Te and ne may also affected the character of the plasma in terms of its reactivity.
This study synthesized collagen-chitosan/PVA nanofiber composites using the electrospinning method. Characterizations included Fourier transform infrared spectroscopy (FTIR) and surface morphology using scanning electron microscopy (SEM). Investigations were carried out on tensile strength, degradation rate, and antibacterial test. It was found that the functional groups C–H, –OH, C–O, C–N, and N–H were suitable for PVA, collagen, and chitosan materials. The SEM showed that increasing the PVA composition caused a change in fiber diameter ranging from 34.64 to 71.63 nm. The tensile strength results show that the smallest nanofiber diameter has the highest ultimate strength value of 5.6 ± 0.4 MPa. In addition, it was found that the rate of degradation was directly proportional to the increase in concentration. Antibacterial activity test was carried out using two types of bacteria, namely gram-positive bacteria S. aureus and gram-negative bacteria E. coli. The results showed that the collagen-chitosan/PVA nanofiber composite had a diameter of antibacterial inhibition for E. coli and S. aureus bacteria, respectively.
The thickness and roughness of metal layers substantially affect the performance of surface plasmon resonance (SPR)-based sensors. The deposition methods, control parameters, and substrate characteristics influence the layer thickness and roughness. This study investigates the SPR characteristics of a polished optical fiber surface coated with gold (Au) metal of different thicknesses. The Au layer is deposited via the thermal evaporation method, and its thickness is varied by controlling the deposition time (3–6 min). A proportionality relationship between thickness and deposition time is observed. Island-shaped structures in gold (Au) morphology are formed due to low adhesion to the substrate. The shape of this island creates gaps in the layer, causing scattering. In addition, the roughness on the gold surface triggers the Localized Surface Plasmon Resonance (LSPR) phenomenon. As a result, the measured dielectric characteristics differ from the reference. The SPR curve calculation simulation was carried out based on reference optical parameters and measurement results by an ellipsometer, which were then compared with experiments. The obtained results show that the substrate roughness, morphology, and thickness of the Au layer play an essential role in determining the characteristics of the SPR curve in a fiber optic plasmonic sensor. As a result, in basic experiments, the sample with an Au thickness of 27.37 nm (deposition time = 3 min) shows better characteristics (half-maximum full width, minimum transmittance, and resonance wavelength) compared with the sample with an Au thickness of 53.97 nm (deposition time = 4 min), Although 53.97 nm is the optimal thickness from the simulation using reference optical parameters (smooth substrate surface and smooth gold layer).