Solution-processed organic–inorganic hybrid perovskite solar cells are among the candidates to replace the traditional silicon solar cells due to their excellent power conversion efficiency (PCE). Despite this considerable progress, understanding the properties of the perovskite precursor solution is critical for perovskite solar cells (PSCs) to achieve high performance and reproducibility. However, the exploration of perovskite precursor chemistry and its effects on photovoltaic performances has been limited thus far. Herein, we modified the equilibrium of chemical species inside the precursor solution using different photoenergy and heat pathways to identify the corresponding perovskite film formation. The illuminated perovskite precursors exhibited a higher density of high-valent iodoplumbate species, resulting in the fabricated perovskite films with reduced defect density and uniform distribution. Conclusively, the perovskite solar cells prepared by the photoaged precursor solution had not only improved PCE but also enhanced current density, confirmed by device performance, conductive atomic force microscopy (C-AFM), and external quantum efficiency (EQE). This innovative precursor photoexcitation is a simple and effective physical process for boosting perovskite morphology and current density.
28 August 2014 in International Journal of Photoenergy
Intrinsic hydrogenated amorphous silicon oxide (i-a-SiO:H) films were used as front and rear buffer layers in crystalline silicon heterojunction (c-Si-HJ) solar cells. The surface passivity and effective lifetime of these i-a-SiO:H films on an n-type silicon wafer were improved by increasing the CO2/SiH4ratios in the films. Using i-a-SiO:H as the front and rear buffer layers in c-Si-HJ solar cells was investigated. The front i-a-SiO:H buffer layer thickness and the CO2/SiH4ratio influenced the open-circuit voltage, fill factor (FF), and temperature coefficient (TC) of the c-Si-HJ solar cells. The highest total area efficiency obtained was 18.5% mV, mA/cm2, and. The TC normalized for this c-Si-HJ solar cell efficiency was −0.301%/°C.