The concept of “high entropy” was first proposed while exploring the unknown center of the metal alloy phase diagram, and then expanded to oxides. The colossal dielectric constant found on the bulk high-entropy oxides (HEOs) reveals the potential application of the high-entropy oxides in the dielectric aspects. Despite the fact that known HEO thin films have not been reported in the field of dielectric properties so far, with the high-entropy effects and theoretical guidance of high entropy, it is predictable that they will be discovered. Currently, researchers are verifying that appropriately increasing the oxygen content in the oxide, raising the temperature and raising the pressure during preparation have an obvious influence on thin films’ resistivity, which may be the guidance on obtaining an HEO film large dielectric constant. Finally, it could composite a metal–insulator–metal capacitor, and contribute to sensors and energy storage devices’ development; alternatively, it could be put into application in emerging thin-film transistor technologies, such as those based on amorphous metal oxide semiconductors, semiconducting carbon nanotubes, and organic semiconductors.
Optical detection is of great significance in various fields such as industry, military, and medical treatment, especially ultraviolet (UV) photodetectors. Moreover, as the demand for wearable devices continues to increase, the UV photodetector, which is one of the most important sensors, has put forward higher requirements for bending resistance, durability, and transparency. Tin oxide (SnO2) has a wide band gap, high ultraviolet exciton gain, etc., and is considered to be an ideal material for preparing UV photodetectors. At present, SnO2-based UV photodetectors have a transparency of more than 70% in the visible light region and also have excellent flexibility of 160% tensile strain. Focusing on SnO2 nanostructures, the article mainly summarizes the progress of SnO2 UV photodetectors in flexibility and transparency in recent years and proposes feasible optimization directions and difficulties.
Flexible and fully transparent thin film transistors (TFT) were fabricated via room temperature processes. The fabricated TFT on the PEN exhibited excellent performance, including a saturation mobility (μsat) of 7.9 cm2/V·s, an Ion/Ioff ratio of 4.58 × 106, a subthreshold swing (SS) of 0.248 V/dec, a transparency of 87.8% at 550 nm, as well as relatively good stability under negative bias stress (NBS) and bending stress, which shows great potential in smart, portable flexible display, and wearable device applications.
Flexible electronic devices have received great attention in the fields of foldable electronic devices, wearable electronic devices, displays, actuators, synaptic bionics and so on. Among them, high-performance flexible memory for information storage and processing is an important part. Due to its simple structure and non-volatile characteristics, flexible resistive random access memory (RRAM) is the most likely flexible memory to achieve full commercialization. At present, the minimum bending radius of flexible RRAM can reach 2 mm and the maximum ON/OFF ratio (storage window) can reach 108. However, there are some defects in reliability and durability. In the bending process, the cracks are the main cause of device failure. The charge trap sites provided by appropriate doping or the use of amorphous nanostructures can make the conductive filaments of flexible RRAM steadier. Flexible electrodes with high conductivity and flexible dielectric with stable storage properties are the main development directions of flexible RRAM materials in the future.
The praseodymium-doped indium-zinc-oxide (PrIZO) thin film transistor (TFT) shows broad application prospects in the new generation of display technologies due to its high performance and high stability. However, traditional device performance evaluation methods need to be carried out after the end of the entire preparation process, which leads to the high-performance device preparation process that takes a lot of time and costs. Therefore, there is a lack of effective methods to optimize the device preparation process. In this paper, the effect of sputtering oxygen partial pressure on the properties of PrIZO thin film was studied, and the quality of PrIZO thin film was quickly evaluated by the microwave photoconductivity decay (µ-PCD) method. The μ-PCD results show that as the oxygen partial pressure increases, the peak first increases and then decreases, while the D value shows the opposite trend. The quality of PrIZO thin film prepared under 10% oxygen partial pressure is optimal due to its low localized defect states. The electric performance of PrIZO TFTs prepared under different oxygen partial pressures is consistent with the μ-PCD results. The optimal PrIZO TFT prepared under 10% oxygen partial pressure exhibits good electric performance with a threshold voltage (Vth) of 1.9 V, a mobility (µsat) of 24.4 cm2·V−1·s−1, an Ion/Ioff ratio of 2.03 × 107, and a subthreshold swing (SS) of 0.14 V·dec−1.
Silver nanowire (AgNW) conductive film fabricated by solution processing was investigated as an alternative to indium tin oxide (ITO) in flexible transparent electrodes. In this paper, we studied a facile and effective method by electrodepositing Al2O3 on the surface of AgNWs. As a result, flexible transparent electrodes with improved stability could be obtained by electrodepositing Al2O3. It was found that, as the annealing temperature rises, the Al2O3 coating layer can be transformed from Al2O3·H2O into a denser amorphous state at 150 °C. By studying the increase of electrodeposition temperature, it was observed that the transmittance of the AgNW–Al2O3 composite films first rose to the maximum at 70 °C and then decreased. With the increase of the electrodeposition time, the figure of merit (FoM) of the composite films increased and reached the maximum when the time was 40 s. Through optimizing the experimental parameters, a high-stability AgNW flexible transparent electrode using polyimide (PI) as a substrate was prepared without sacrificing optical and electrical performance by electrodepositing at −1.1 V and 70 °C for 40 s with 0.1 mol/L Al(NO3)3 as the electrolyte, which can withstand a high temperature of 250 °C or 250,000 bending cycles with a bending radius of 4 mm.