A novel manufacturing approach was used to fabricate metallic scaffolds. A calibration of the laser cutting process was performed using the kerf width compensation in the calculations of the tool trajectory. Welding defects were studied through X-ray microtomography. Penetration depth and width resulted in relative errors of 9.4%, 1.0%, respectively. Microhardness was also measured, and the microstructure was studied in the base material. The microhardness values obtained were 400 HV, 237 HV, and 215 HV for the base material, HAZ, and fusion zone, respectively. No significant difference was found between the microhardness measurement along with different height positions of the scaffold. The scaffolds’ dimensions and porosity were measured, their internal architecture was observed with micro-computed tomography. The results indicated that geometries with dimensions under 500 µm with different shapes resulted in relative errors of ~2.7%. The fabricated scaffolds presented an average compressive modulus ~13.15 GPa, which is close to cortical bone properties. The proposed methodology showed a promising future in bone tissue engineering applications.
14 January 2026 in Progress in Additive Manufacturing
This study investigates the influence of laser polishing (LP) as a post-processing method for enhancing the surface quality of Laser Powder Bed Fusion (LPBF) components. Cylindrical specimens were manufactured using LPBF processing parameters (i.e., laser power of 150 and 170 W, and point distance of 20 and 30 μm) for a range of specific energies between 5.0 and 8.5 J/mm2. After this process, LP treatment was performed on the top surfaces at energy densities ranging from 0.142 to 0.475 J/mm. Surface characterization was performed by measuring surface roughness (Ra, Rz), height, and surface topography quality. Apparent density and cross-sectional surface porosity of the LPBF were quantified. The results indicated that higher specific energy values (> 7.5 J/mm2) during the LPBF process produced samples with lower surface roughness, reduced porosity (1.42–1.97%), and increased density (7.30–7.36 g/cm2). LP post-processing demonstrated that an energy per unit length of 0.225 J/mm was most effective at reducing the ten-point mean roughness and height across all sample types. The maximum reduction in ten-point surface roughness achieved was 52.5% (from 70.71 μm to 33.58 μm) in samples with a specific energy of 5.33 J/mm2. Microhardness measurements revealed that LP slightly softened the near-surface region (≈ 4 μm depth) in high-porosity samples, while samples with porosity below 2% exhibited higher and more uniform hardness profiles up to 1000 μm. Our findings reveal that LP effectiveness is strongly dependent on initial surface quality and porosity of LPBF components, emphasizing the importance of post-processing stages for achieving a superior surface finish.