The dip coating process is one of the recognized techniques used to generate polymeric coatings on stents in an easy and low-cost way. However, there is a lack of information about the influence of the process parameters of this technique on complex geometries such as stents. This paper studies the dip coating process parameters used to provide a uniform coating of PLA with a 4–10 µm thickness. A stainless-steel tube (AISI 316L) was laser-cut, electropolished, and dip-coated in a polylactic acid (PLA) solution whilst changing the process parameters. The samples were characterized to examine the coating’s uniformity, thickness, surface roughness, weight, and chemical composition. FTIR and Raman investigations indicated the presence of PLA on the stent’s surface, the chemical stability of PLA during the coating process, and the absence of residual chloroform in the coatings. Additionally, the water contact angle was measured to determine the hydrophilicity of the coating. Our results indicate that, when using entry and withdrawal speeds of 500 mm min−1 and a 15 s immersion time, a uniform coating thickness was achieved throughout the tube and in the stent with an average thickness of 7.8 µm.
Magnesium-based coronary stents have gained significant interest due to their excellent biocompatibility, biodegradability, and mechanical properties. However, a key limitation of magnesium in biomedical applications is its low corrosion resistance, which compromises its structural integrity and mechanical strength over time. Polymeric coatings can overcome this challenge, enhancing magnesium-based implants’ corrosion resistance and overall performance. This study applied a polylactic acid (PLA) nanofiber coating to WE43 magnesium (Mg) stents via electrospinning to reduce their corrosion rate. Both uncoated and coated stents underwent in vitro immersion tests in Hank’s solution for 1, 3, 7, and 14 days. The effectiveness of the PLA coating was evaluated through morphological analysis, chemical composition assessment, corrosion behavior (weight change), magnesium ion release, and in vitro biocompatibility. The corrosion observed in the uncoated WE43 stents indicates that protective coatings are necessary to regulate degradation rates over extended implantation periods. The results demonstrated that coated stents exhibited improved performance, maintaining the integrity of the PLA coating for up to 14 days. The coated stents demonstrated reduced surface damage and lower weight loss resulting from lower magnesium release. In our study, the coated stents demonstrated a reduced corrosion rate (0.216 ± 0.013 mm/year) compared with the uncoated stents (0.312 ± 0.010 mm/year), both after 14 days. Additionally, in vitro biocompatibility results confirmed the non-toxic nature of PLA-coated stents, which enhances cellular proliferation and contributes to a more favorable environment for vascular healing. These findings suggest that PLA coatings can effectively prolong the functional durability of WE43 Mg stents, offering a promising solution for enhancing the performance of biodegradable stents in cardiovascular applications.
26 February 2026 in Progress in Additive Manufacturing
This study investigates the influence of laser polishing (LP) as a post-processing method for enhancing the surface quality of Laser Powder Bed Fusion (LPBF) components. Cylindrical specimens were manufactured using LPBF processing parameters (i.e., laser power of 150 and 170 W, and point distance of 20 and 30 μm) for a range of specific energies between 5.0 and 8.5 J/mm2. After this process, LP treatment was performed on the top surfaces at energy densities ranging from 0.142 to 0.475 J/mm. Surface characterization was performed by measuring surface roughness (Ra, Rz), height, and surface topography quality. Apparent density and cross-sectional surface porosity of the LPBF were quantified. The results indicated that higher specific energy values (> 7.5 J/mm2) during the LPBF process produced samples with lower surface roughness, reduced porosity (1.42–1.97%), and increased density (7.30–7.36 g/cm2). LP post-processing demonstrated that an energy per unit length of 0.225 J/mm was most effective at reducing the ten-point mean roughness and height across all sample types. The maximum reduction in ten-point surface roughness achieved was 52.5% (from 70.71 μm to 33.58 μm) in samples with a specific energy of 5.33 J/mm2. Microhardness measurements revealed that LP slightly softened the near-surface region (≈ 4 μm depth) in high-porosity samples, while samples with porosity below 2% exhibited higher and more uniform hardness profiles up to 1000 μm. Our findings reveal that LP effectiveness is strongly dependent on initial surface quality and porosity of LPBF components, emphasizing the importance of post-processing stages for achieving a superior surface finish.