The results of the high-field technique for obtaining and testing the carbyne strength in situ are presented. By using molecular dynamics simulation and ab initio calculations, a comprehensive analysis of the results is executed. High-field technique for experimental measurement of the carbyne strength in situ is briefly described. It is shown that the technique used gives a lower estimation for strength of carbyne, which equals 251 GPa at T = 77 K. This value is close to the strength 7.85 nN (250 GPa) of contact atomic bond between carbyne and graphene sheet, from which the monatomic chain is pulled. The strength of carbyne itself is determined by strength of an edge atomic bond and it is ≈ 12.35 nN (393 GPa) at T = 0 K. For carbynes containing more than 10 to 12 atoms, the coefficient of elasticity (k Y = 145.40 nN) and the elastic modulus (Y = 4631 GPa) are ascertain.
The atomic structure and mechanical properties of the carbyne (monatomic linear chains), containing from 2 to 21 carbon atoms, are theoretically investigated by ab-initio methods. We demonstrate the existence of a stable cumulene structure in the inner part of chains with the number of atoms . We present a general stress-strain diagram of chains until the moment when they break, which enables to determine their strength, elasticity, and fragility. These diagrams can be utilized to calibrate empirical potentials, especially for large deviations of the atoms from the equilibrium positions. For chains with , the relationship between the strength of the chain and the binding energy of the edge atom in the chain is established. The existence of scale-effect and “even-odd” effect for such properties as strength, elasticity, and fragility is observed. We demonstrate that the five-atom carbon chains show the maximum strength value.
1 April 2006 in Theoretical and Applied Fracture Mechanics
The intrinsic strength of freestanding carbon atomic chains was measured by in situ high-field mechanical testing of carbon atomic chains carried out inside a field-ion microscope. The determined breaking field strength corresponds to a tensile strength of carbon atomic chains at 5 K equal to 245 GPa. Carbon atomic chains also show exceptionally high-evaporation stability in electric fields up to 259 V/nm. The tensile strength of linear carbon chains significantly exceeds the tensile strength of known two-dimensional and three-dimensional carbon materials, including carbon nanotubes and graphene. Our results can be considered as direct experimental evidence for Pauling's prediction of bond stiffening with reduced atomic bond order.
1 August 2009 in Science and Technology of Advanced Materials
The strength of Mo nanorods was measured under uniaxial tension. Tensile tests of 〈 110〉-oriented single-crystalline molybdenum rod-shaped specimens with diameters from 25 to 90 nm at the apex were conducted inside a field-ion microscope (FIM). The nanocrystals were free from dislocations, planar defects and microcracks, and exhibited the plastic mode of failure under uniaxial tension with the formation of a chisel-edge tip by multiple gliding in the [Formula: see text] and [Formula: see text] deformation systems. The experimental values of tensile strength vary between 6.3 and 19.8 GPa and show a decrease with increasing nanorod diameter. A molecular dynamic simulation of Mo nanorod tension also suggests that the strength decreases from 28.8 to 21.0 GPa when the rod diameter increases from 3.1 to 15.7 nm. The maximum values of experimental strength are thought to correspond to the inherent strength of Mo nanocrystals under uniaxial tension (19.8 GPa, or 7.5% of Young's modulus).