One of the key issues limiting the application of Al-Mg-Zn-Cu alloys in the automotive industry is forming at a low cost. Isothermal uniaxial compression was accomplished in the range of 300–450 °C, 0.001–10 s−1 to study the hot deformation behavior of an as-cast Al-5.07Mg-3.01Zn-1.11Cu-0.01Ti alloy. Its rheological behavior presented characteristics of work-hardening followed by dynamic softening and its flow stress was accurately described by the proposed strain-compensated Arrhenius-type constitutive model. Three-dimensional processing maps were established. The instability was mainly concentrated in regions with high strain rates or low temperatures, with cracking being the main instability. A workable domain was determined as 385–450 °C, 0.001–0.26 s−1, in which dynamic recovery (DRV) and dynamic recrystallization (DRX) occurred. As the temperature rose, the dominant dynamic softening mechanism shifted from DRV to DRX. The DRX mechanisms transformed from continuous dynamic recrystallization (CDRX), discontinuous dynamic recrystallization (DDRX), and particle-stimulated nucleation (PSN) at 350 °C, 0.1 s−1 to CDRX and DDRX at 450 °C, 0.01 s−1, and eventually to DDRX at 450 °C, 0.001 s−1. The eutectic T-Mg32(AlZnCu)49 phase facilitated DRX nucleation and did not trigger instability in the workable domain. This work demonstrates that the workability of as-cast Al-Mg-Zn-Cu alloys with low Zn/Mg ratios is sufficient for hot forming.
The design of the overall thickness and thickness ratio in multilayered composites is vital because it affects interfacial microstructures and mechanical properties. These elements are significant in the application of multilayered composites in diverse scenarios. This study systematically investigated the interfacial microstructure, mechanical properties, and fracture mechanisms of Cu/Al/Cu trilayered composites with varying overall thicknesses and copper thickness ratios. The microstructure results showed that the distribution and thickness of intermetallic compounds (IMCs) at the Cu/Al interface changed significantly with different thickness designs. As the Cu thickness ratio increased from 20% to 35%, the intermetallic layer transitioned from a continuous structure to a fragmented one in both the 1 mm and 2 mm composites. Additionally, the bonding mechanism evolved from primarily metallurgical bonding to a combination of metallurgical and mechanical bonding. In the 4 mm composite with a 35% Cu thickness ratio, the interfacial intermetallic layer comprised three sublayers identified as Al4Cu9, AlCu, and Al2Cu. Tensile results indicated that increasing the Cu thickness ratio markedly enhanced strength and ductility: the 1 mm composite showed increases of 22.3% in ultimate tensile strength and 70.9% in elongation, while the 2 mm composite exhibited increases of 32.4% and 38.7%, respectively. In contrast, increasing the overall thickness had only a limited effect. Fractography revealed ductile fracture features in both the Al and Cu layers, characterized by more compact interfaces, deeper dimples, and more pronounced tear ridges at higher Cu thickness ratios. These findings demonstrate that optimizing the Cu thickness ratio is an effective strategy for enhancing interfacial bonding strength and overall mechanical performance in Cu/Al/Cu composites.