In this study, the interactions of magnesium (Mg) atom and Mg(001) surface with different metal-atom-doped graphene were investigated using a density functional theory (DFT) method. For the interactions of magnesium with Al-, Mn-, Zn-, and Zr-doped and intrinsic graphene, it was found that the magnesium atoms were physisorbed into the hollow sites of the intrinsic graphene with only the smallest interaction energy (approximately −1.900 eV). However, the magnesium atoms tended to be chemisorbed on the doped graphene, which exhibited larger interaction energies and charge transfers. Additionally, the Zn-doped graphene displayed the largest interaction energy with the Mg atom (approximately −3.833 eV). For the interactions of Mg(001) with Al-, Mn-, Zn-, and Zr-doped and intrinsic graphene (intrinsic and doped graphene/Mg interface), doped atoms interacted with a Mg layer to make graphene wrinkle, resulting in a higher specific surface area and better stability. Mg–C chemical bonds were formed at the Al-, Zn-, and Zr-doped interface, and Mg–Mn chemical bonds were formed at the Mn-doped interface. This study provided the fundamental research for future research into doped atoms on graphene reinforced magnesium matrix composites.
The two-sheet hollow structure of the 1420 Al-Li alloy was prepared by the method of superplastic forming and diffusion bonding. The interface combination status of the diffusion bonding region and the microstructure of the superplastic forming region were observed by an optical microscope. The thickness distribution of the superplastic forming region was measured by an ultrasonic thickness meter machine, the defect detection was tested by X-ray nondestructive inspection, and the failure modes of the samples were analyzed. The results showed that the two-sheet hollow structure of the 1420 Al-Li alloy was prepared successfully, the structure was integrated, and there were no shape defects such as pit, wrinkle, and collapse. The structure shape was almost attached to the die completely, and the thickness was almost uniform distribution. The no deforming area of the two-sheet hollow structure of the 1420 Al-Li alloy was a long strip, rolled microstructure, while the grains near the round corner area were equiaxed states resulting from dynamic recrystallization. The improper control of the superplastic gas pressure in the forming process would lead to the tearing or the die-attaching failure for the two-sheet hollow structure of the 1420 Al-Li alloy.
The high uniform magnetic field combined with pre-deformation and vacuum heat treatment processing is designed for improving the diffusion bonding properties of the 1420 Al-Li alloy. Serial magneto-thermal coupling treatment experiments of 1420 Al-Li alloy and the pure aluminium diffusion couple, together with the gallium interlayer, is carried out in a superconducting high magnetic field device. Various parameter combinations are used to produce different samples on which interface organization and connection performance are studied. Electron microscopic analysis reveals various interface topographies and fracture morphologies after shear strength tests. Influence of diffusion bonding temperature on element diffusion under a high uniform magnetic field is investigated. The diffusion activation energy of Mg element in pure aluminum under a 12 T magnetic field is calculated in this paper. It is found that the bonding quality and bonding performance of the interface are improved greatly after heat treatment with a strong magnetic field, and the bonding temperature is an important factor affecting the interface bonding and bonding strength. The diffusion coefficient of the Mg element in the 1420 Al-Li alloy to L2 pure aluminum increases with the increase of diffusion bonding temperature. Reducing the activation energy of elemental diffusion is beneficial to atomic diffusion.
Based on the working principle of magnetorheological fluid damping, in this paper, a set of squeezing mode Magneto-rheological Fluid (MRF) dampers is designed for drilling vibration suppression in deep hole machines. Elaborate analysis of the correlativity between the dynamic morphology trajectory of the machined hole surface, the vibration of the drilling tool-shaft, and the theoretical derivation of the damping force, is put forward in accordance with the Bingham model and Euler-Bernoulli beam Equation. Simultaneously, the contrast analysis of the vibration suppression effect is carried out through the drilling experiments with and without an MRF damper. In addition, a series of measurements on the vibration characteristics of the drilling shaft, the drilling tool and the guide surface wear patterns, and the machine hole surface are analyzed, respectively. Both the drilling experiments and theory studies have revealed that the strength of the magnetic field changed with the drill shaft at different levels of vibration. The MRF damper could suppress the vibration with nonlinear characteristics initiatively and instantaneously, by variable damping, which can eventually improve the surface roughness. In addition, according to the phenomenon of tool tipping, the breakage of the guide bars and the machine hole surface deduces the condition of the vibration effect objectively.
The unique cutting–burnishing coupling effect in BTA deep hole drilling generates a high-hardness and -brittleness white layer (ultrafine martensitic layer), which will degrade component performance and accelerate tool wear. This work investigated the formation mechanism and the mechanical properties of the white layer generated in three distinct regions (the cutting edge radius zone, cutting–burnishing corner zone, and guide pad edge zone) through nanoindentation, SEM and BSE. The microstructure and thickness of the white layer under different feedrates are investigated. The correlations between the white layer, the structure of guide pads, and wear behaviors of the TiN- and TiCN/Al2O3-coated guide pads are revealed. Variations in hardness are observed across different zones. The white layer undergoes a soft-to-hard transition due to rapid quenching and the cutting–burnishing effect at the sharp corner. The highest hardness (9.758 GPa) was observed in the guide pad zone, accompanied by grain refinement. The chamfered TiN-coated guide pad exhibits superior wear resistance but suffers fatigue cracking and adhesive wear in the initial guiding zone. The TiCN/Al2O3-coated pad with rounded corners experiences brittle spalling in the mid-to-rear guiding zone. These findings enhance the understanding of the white layer formation in deep hole drilling and provide a foundation for tool optimization.