The fundamental processes of nucleation and crystallization are widely observed in systems relevant to material synthesis and biomineralization; yet most often, their mechanism remains unclear. In this study, we unravel the discrete stages of nucleation and crystallization of Fe3(PO4)2·8H2O (vivianite). We experimentally monitored the formation and transformation from ions to solid products by employing correlated, time-resolved in situ and ex situ approaches. We show that vivianite crystallization occurs in distinct stages via a transient amorphous precursor phase. The metastable amorphous ferrous phosphate (AFEP) intermediate could be isolated and stabilized. We resolved the differences in bonding environments, structure, and symmetric changes of the Fe site during the transformation of AFEP to crystalline vivianite through synchrotron X-ray absorption spectroscopy at the Fe K-edge. This intermediate AFEP phase has a lower water content and less distorted local symmetry, compared to the crystalline end product vivianite. Our combined results indicate that a nonclassical, hydration-induced nucleation and transformation driven by the incorporation and rearrangement of water molecules and ions (Fe2+ and PO43-) within the AFEP is the dominating mechanism of vivianite formation at moderately high to low vivianite supersaturations (saturation index ≤ 10.19). We offer fundamental insights into the aqueous, amorphous-to-crystalline transformations in the Fe2+-PO4 system and highlight the different attributes of the AFEP, compared to its crystalline counterpart.
Inconel 718 is a precipitation strengthened, nickel-based super alloy of interest for the Additive Manufacturing (AM) of low volume, complex parts to reduce production time and cost compared to conventional subtractive processes. The AM process involves repeated rapid melting, solidification and reheating, which exposes the material to non-equilibrium conditions that affect elemental segregation and the subsequent formation of solidification phases, either beneficial or detrimental. These variations are difficult to characterize due to the small length scale within the micron sized melt pool. To understand how the non-equilibrium conditions affect the initial solidification phases and their critical temperatures, a multi-length scale, multi modal approach has been taken to evaluate various methods for identifying the initial phases formed in the as-built Inconel 718 produced by laser-powder bed fusion (L-PBF) additive manufacturing (AM). Using a range of characterization tools from the bulk differential thermal analysis (DTA) and x-ray diffraction (XRD) to spatially resolved images using a variety of electron microscopy tools, a better understanding is obtained of how these minor phases can be properly identified regarding the amount and size, morphology and distribution. Using the most promising characterization techniques for investigation of the as-built specimens, those techniques were used to evaluate the specimens after various heat treatments. During the sequence of heat treatments, the initial as-built dendritic structures recrystallized into well-defined grains whose size was dependent on the temperature. Although the resulting strength was similar in all heat treated specimens, the elongation increased as the grain size was refined due to differences in the precipitated phase distribution and morphology.
6 November 2013 in The Journal of Chemical Physics
The internal friction of hydrated soda-lime-silica glasses with total water content (CW) up to 1.9 wt. % was studied by dynamic mechanical analysis (DMA) using temperature-frequency sweeps from 723 K to 273 K and from 1 s−1 to 50 s−1. Total water content and concentrations of H2O molecules ( ) and OH groups (COH) in the DMA specimens were determined by infrared spectroscopy. For low water contents (CW ≈ COH < 0.25 wt. %) two discrete internal friction peaks below the glass transition (α relaxation) were assigned to the low-temperature motion of alkali ions (γ relaxation) and cooperative movements of dissimilar mobile species under participation of OH at higher temperature (βOH relaxation). For large water contents (CW > 1 wt. %), where significant amounts of molecular water are evident ( > 0.15 wt. %), however, internal friction spectra change unexpectedly: the βOH peak heights saturate and a low temperature shoulder appears on the β-relaxation peak. This emerging relaxation mode ( relaxation) was assigned to the motions of H2O molecules. relaxation was found to be faster than βOH but slower than γ relaxation. Activation energy of the different relaxation modes increased in the order γ < < βOH < α.
1 October 2019 in Journal of Non-Crystalline Solids
The development of new glasses is often hampered by inefficient trial‐and‐error approaches. The traditional glass manufacturing process is not only time‐consuming, but also difficult to reproduce with inevitable variations in process parameters. These challenges are addressed by implementing an ontology‐based digital infrastructure coupled with a robotic melting system. This system facilitates high‐throughput glass synthesis and ensures the collection of consistent process data. In addition, the digital infrastructure includes machine learning models for predicting glass properties and a tool for extracting patent information. Current glass databases have significant gaps in the relationships between compositions, process parameters, and properties due to inconsistent studies and nonconforming units. In addition, process parameters are often omitted, and even original literature references provide limited information. By continuously expanding the database with consistent, high‐quality data, it is aimed to fill these gaps and accelerate the glass development process.