The article is devoted to modification of the impact devices of Leeb hardness testers for the implementation of the dynamic instrumented indentation method. The results obtained made it possible to construct a load–displacement curve using primary EMF signals and made it possible to determine the values of the dissipated and elastic impact body energy, the maximal load of indentation, the maximal and residual penetration depth and the geometric parameters of the indentation region, namely the contact area of the indenter with the surface and the volume of the displaced material. The listed parameters of the indentation process allow us to measure the contact and volume hardness, the elastic modulus and the yield strength of test objects with portable hardness testers.
The issues of improving the accuracy of estimating the indenter motion parameters in the primary converter of a dynamic instrumented indentation device using two counter-connected coil windings (differential coil) are considered. The calculation of the characteristics of the primary converter is based on computer modeling and solving the problem of step-by-step conditional optimization of the relative dimensions of the striker magnet and coil. The results of a study of a primary converter with a differential coil (comparative estimates of the recorded signal — EMF and the dynamic modulus of elasticity of steel St.3) in relation to the existing primary sensor converter of the TPTS-7 device, which showed its advantage.
The study was carried out as part of the development of a non-destructive method for measuring the mechanical properties of metals and alloys based on the dynamic instrumented indentation method. The purpose of this work is to study the possibility of measuring the modulus of elasticity using a modified Leeb hardness tester. The experiment was carried out on samples of 20X25H20C2, 20X23H18, BpA9Zh4H4Mts1 alloys.
The results of a comparative analysis of three methods for calculating the elastic modulus during dynamic instrumental indentation are presented: in accordance with GOST R 56474, GOST R 8.748 and the proposed original method based on data from optical analysis of the indentation using prepared samples of alloys 20Х25Н20С2, 20Х23Н18 and BrANZhNMts9-4-4- 1.