In this study, a nanostructured TiO2 coating was successfully prepared on a large-scale titanium plate by a simple one-step surface mechanical alloying (SMA) treatment. The coating was characterised to determine the morphological and composition changes with SMA. The coating was ∼60 μm thick and composed of 5 nm diameter rutile TiO2 particles. The photocatalytic activity of the nanostructured TiO2 coating was studied via the ultraviolet–visible (UV–vis) decolorisation of aqueous rhodamine-B. The results showed that the photocatalytic degradation effect in 5 h of the φ30 mm nanostructured TiO2 coating was comparable to that of 20 mg raw TiO2 under similar UV–visible light irradiation. One-step SMA was demonstrated as an appropriate method to produce a high-performance photocatalytic plate.
It was demonstrated that the mechanical shot peening (MSP) technique was a viable way to obtain a nanocrystalline layer on a large size pure titanium plate due to the MSP provided for severe plastic deformation (SPD) of surface high velocity balls impacting. The MSP effects of various durations in producing the surface nanocrystalline layer was characterized by optical microscope (OM), X-ray diffraction (XRD), transmission electron microscope (TEM), and Vickers micro-hardness tester. The results showed that the thickness of the SPD layer gradually increased with the MSP processing time increase, but saturated at 230 μm after 30 min. The average grain size was refined to about 18.48 nm in the nanocrystalline layer. There was equiaxed grain morphology with random crystallographic orientation in the topmost surface. By comparing with the nanocrystalline layer, acquired by surface mechanical attrition treatment (SMAT), the microstructure and properties of the nanocrystalline layer acquired by MSP was evidently superior to that of the SMAT, but the production time was cut to about a quarter of the time used for the SMAT method.
Surface mechanical attrition treatment (SMAT) is an effective method to accelerate the nitriding process of metallic materials. In this work, a novel technique named surface nano-alloying (SNA) was developed on the basis of surface mechanical attrition treatment, which was employed as a pretreatment for the nitriding of low carbon steel materials. The microstructure and surface properties of treated samples were investigated by SEM, XRD, TEM and the Vickers hardness test. Experimental results showed that a surface alloying layer (Cr element) of about 10–20 μm in thickness was formed on the low carbon steel sample after the surface nano-alloying treatment. After nitriding for the SNA sample, a complex compound layer composed of Fe2–3N, FeCr and Cr2N phases was fabricated. Moreover, the thickness of this compound layer was about 50 μm. Meanwhile, both the surface hardness and wear resistance of the SNA nitrided sample are better that those of the SMAT nitrided sample. This work offers a new approach for improving the nitriding process of steel materials.
The light weight, electrical conductivity, environmental friendliness, and high mechanical properties of graphene/PEKK composites make them popular in biomedical, electronic component and aerospace fields. However, the compaction density and carbonization of the specimen influence the microstructure and conductivity of the graphene/PEKK composite prepared by in situ polymerization, so electromagnetic-assisted molding was used to manufacture products to avoid carbonization and enhance the compaction density. The effects of different discharge voltages on the microstructure of the formed graphene/PEKK specimens were compared. Increasing the discharge voltage will lead to a closer distribution of flake graphene in the matrix to improve the compaction density, mechanical performance and conductivity. At the same time, the numerical analysis model was validated by comparison with the compaction density of the experimental results. Based on this research, the stress/strain distribution on the specimen was obtained with increasing discharge voltages.