In this paper, a nanocrystalline surface layer without impurities was fabricated on Ti-6Al-4V alloy by means of surface mechanical attrition treatment (SMAT). The grain size in the nanocrystalline layer is about 10 nm and grain morphology displays a random crystallographic orientation distribution. Subsequently, the low-temperature boriding behaviors (at 600 °C) of the SMAT sample, including the phase composition, microstructure, micro-hardness, and brittleness, were investigated in comparison with those of coarse-grained sample borided at 1100 °C. The results showed that the boriding kinetics could be significantly enhanced by SMAT, resulting in the formation of a nano-structured boride layers on Ti-6Al-4V alloy at lower temperature. Compared to the coarse-grained boriding sample, the SMAT boriding sample exhibits a similar hardness value, but improved surface toughness. The satisfactory surface toughness may be attributed to the boriding treatment that was carried out at lower temperature.
The thick titanium nitrides coating was fabricated on LZ91 alloy by surface mechanical nano-alloying (SMNAT) combined with gas nitriding. Experimental results showed that a nanostructured titanium coating with thickness of 50–80 μm was formed on surface of LZ91 alloy by SMNAT with pure titanium powders for 30 min. By adding of the aluminium powders into titanium powders during the SMNAT, a thicker Ti-Al composite coating with improved continuity and uniformity was obtained. After nitriding at 450°C, the whole Ti and Ti-Al coating were successfully nitrided. The surface layer of nitrided Ti coated sample is mainly composed of TiN, Ti2N, TiN0.3, TiN0.61 and Ti4N2.33 phases and the surface layer of nitrided Ti-Al coated sample is composed of Ti2N, TiN0.9, TiN0.3, Ti4N2.33, AlN, Ti3Al2N2 and AlTi2N phases. The hardness measurements demonstrated that the surface hardness of nitrided Ti coated and nitrided Ti-Al coated samples reached to 634 and 734 HV, respectively.
Surface mechanical attrition treatment (SMAT) is an effective method to accelerate the nitriding process of metallic materials. In this work, a novel technique named surface nano-alloying (SNA) was developed on the basis of surface mechanical attrition treatment, which was employed as a pretreatment for the nitriding of low carbon steel materials. The microstructure and surface properties of treated samples were investigated by SEM, XRD, TEM and the Vickers hardness test. Experimental results showed that a surface alloying layer (Cr element) of about 10–20 μm in thickness was formed on the low carbon steel sample after the surface nano-alloying treatment. After nitriding for the SNA sample, a complex compound layer composed of Fe2–3N, FeCr and Cr2N phases was fabricated. Moreover, the thickness of this compound layer was about 50 μm. Meanwhile, both the surface hardness and wear resistance of the SNA nitrided sample are better that those of the SMAT nitrided sample. This work offers a new approach for improving the nitriding process of steel materials.