Thermophysical properties of a carbon-reinforced epoxy composite laminate (T700/M21 composite for aircraft structures) were evaluated using different innovative characterisation methods. Thermogravimetric Analysis (TGA), Simultaneous Thermal analysis (STA), Laser Flash analysis (LFA), and Fourier Transform Infrared (FTIR) analysis were used for measuring the thermal decomposition, the specific heat capacity, the anisotropic thermal conductivity of the composite, the heats of decomposition and the specific heat capacity of released gases. It permits to get input data to feed a three-dimensional (3D) model given the temperature profile and the mass loss obtained during well-defined fire scenarios (model presented in Part II of this paper). The measurements were optimised to get accurate data. The data also permit to create a public database on an aeronautical carbon fibre/epoxy composite for fire safety engineering.
16 April 2008 in Polymers for Advanced Technologies
Intumescent coatings, mainly composed of ammonium polyphosphate, pentaerythritol and melamine, are widely used in the field of fire protection of steel structures. The objective of this study was to investigate how the presence of two different inorganic fillers (titanium dioxide and mineral fibres) will affect the fire performance of an acrylic-based intumescent coating. In both cases, it was observed that the inorganic filler enabled improvement of the fire-protective behaviour of intumescent paints, maintaining their performance for a longer time. The mode of action was attributed to reinforcement of the char due to the presence of the fillers.
The pyrolysis of solid polymeric materials is a complex process that involves both chemical and physical phenomena such as phase transitions, chemical reactions, heat transfer, and mass transport of gaseous components. For modeling purposes, it is important to characterize and to quantify the properties driving those phenomena, especially in the case of flame-retarded materials. In this study, protocols have been developed to characterize the thermal conductivity and the heat capacity of an ethylene-vinyl acetate copolymer (EVA) flame retarded with aluminum tri-hydroxide (ATH). These properties were measured for the various species identified across the decomposition of the material. Namely, the thermal conductivity was found to decrease as a function of temperature before decomposition whereas the ceramic residue obtained after the decomposition at the steady state exhibits a thermal conductivity as low as 0.2 W/m/K. The heat capacity of the material was also investigated using both isothermal modulated Differential Scanning Calorimetry (DSC) and the standard method (ASTM E1269). It was shown that the final residue exhibits a similar behavior to alumina, which is consistent with the decomposition pathway of EVA/ATH. Besides, the two experimental approaches give similar results over the whole range of temperatures. Moreover, the optical properties before decomposition and the heat capacity of the decomposition gases were also analyzed. Those properties were then used as input data for a pyrolysis model in order to predict gasification experiments. Mass losses of gasification experiments were well predicted, thus validating the characterization of the thermo-physical properties of the material.
Polyamide 6 (PA6) is a widely-used polymer that could find applications in various sectors, including home textiles, transportation or construction. However, due to its organic nature, PA6 is flammable, and flame-retardant formulations have to be developed to comply with fire safety standards. Recently, it was proposed to use ammonium sulfamate as an effective flame retardant for PA6, even at low loading content. However, processing issues could occur with this additive considering large-scale production. This paper thus studies the use of another sulfamate salt—guanidine sulfamate (GAS)—and evidences its high efficiency when combined with melamine polyphosphate (MPP) as a flame retardant for PA6. A decrease of the peak of the heat release rate by 30% compared to pure PA6 was obtained using only 5 wt% of a GAS/MPP mixture in a microscale calorimeter. Moreover, PA6 containing the mixture GAS/MPP exhibits a Limiting Oxygen Index (LOI) of 37 vol% and is rated V0 for the UL 94 test (Vertical Burning Test; ASTM D 3801). The mechanisms of degradation were investigated analyzing the gas phase and solid phase when the material degrades. It was proposed that MPP and GAS modify the degradation pathway of PA6, leading to the formation of nitrile end-group-containing molecules. Moreover, the formation of a polyaromatic structure by the reaction of MPP and PA6 was also shown.