Light ion implantation is one of the important procedures of smart cut for SiC-based semiconductor fabrication. This work investigated the surface morphologies and microstructures of single crystal 6H-SiC irradiated by one or both of H2+ and He+ ions at room temperature and then annealed at specific temperatures. Blisters evolved from the coalescence of H nanocracks were formed in the H2+ and He++H2+ irradiated sample surface, while circular ripples originated from the pressure release of helium bubbles after high temperature annealing were formed in the He+ irradiated sample surface. The lateral radius a of the blisters in the irradiated sample with low H2+ fluence was larger than that in the irradiated sample with high H2+ fluence and with He++H2+ ions. About 8–58% of implanted H atoms contributed to the formation of the blisters. Compared with other irradiated samples, the ratio of w0/a and the density of the blisters in the He++H2+ irradiated samples were largest. The stress field of the blisters was simulated using finite element method and the inner pressure in the blisters was also calculated. The corresponding mechanism was analyzed and discussed.

15 December 2017 in Metals
Verified
Journal Article
Open access
PDF file
JLJianxin Lin
Jianxin Lin
GRGuang Ran
Guang Ran
Penghui LeiPenghui Lei
Penghui Lei
CYChao Ye
Chao Ye
SHShilin Huang
Shilin Huang
NLNing Li
Ning Li
The microstructure of Al/B4C metal matrix composites (MMCs) used as neutron absorbers in both dry storage casks and wet storage pools of spent nuclear fuel was analyzed by SEM and TEM. A polishing method of a focused Ga+ ion beam was used to obtain an ideal sample surface with very low roughness, which was used to statistically analyze the distribution characteristics and size factor of B4C particles in the aluminum matrix. The area of B4C particles mainly ranged from 0 to 0.5 μm2, which was the proportion of 64.29%, 86.99% and 76.86% of total statistical results for the Al-15%B4C, Al-25%B4C and Al-30%B4C MMCs, respectively. The average area of B4C particles in the Al-15%B4C, Al-25%B4C and Al-30%B4C MMCs were about 1.396, 0.528 and 1.183 μm2, respectively. The nanoscale precipitates were analyzed by the element mappings in scanning transmission electron microscopy (STEM) mode and electron energy loss spectroscopy (EELS) mode, which included elliptic alloy precipitates with elemental Cu, Cr, Fe and Si, except for Al, and B4C nanoparticles with polygonal shape. The interface characteristics showed that the (021) crystal plane of B4C particle and (111) crystal plane of aluminum matrix grew together. The lattice misfit was about 1.68% for (111)Al//(021)B4C. The corrosion properties and corresponding mechanism of Al/B4C MMCs were investigated in an aqueous solution with 5000 ppm boric acid at 100 °C and atmospheric pressure, which showed that the mass increment rate was first decreased with increasing corrosion time and then increased.

25 October 2017 in Materials
Verified
Journal Article
Open access
PDF file
CYChao Ye
Chao Ye
GRGuang Ran
Guang Ran
WZWei Zhou
Wei Zhou
QSQiang Shen
Qiang Shen
QFQijie Feng
Qijie Feng
JLJianxin Lin
Jianxin Lin
Single crystal 6H-SiC wafers with 4° off-axis [0001] orientation were irradiated with carbon ions and then annealed at 900 °C for different time periods. The microstructure and surface morphology of these samples were investigated by grazing incidence X-ray diffraction (GIXRD), scanning electron microscopy (SEM), and transmission electron microscopy (TEM). Ion irradiation induced SiC amorphization, but the surface was smooth and did not have special structures. During the annealing process, the amorphous SiC was recrystallized to form columnar crystals that had a large amount of twin structures. The longer the annealing time was, the greater the amount of recrystallized SiC would be. The recrystallization volume fraction was accorded with the law of the Johnson–Mehl–Avrami equation. The surface morphology consisted of tiny pieces with an average width of approximately 30 nm in the annealed SiC. The volume shrinkage of irradiated SiC layer and the anisotropy of newly born crystals during annealing process produced internal stress and then induced not only a large number of dislocation walls in the non-irradiated layer but also the initiation and propagation of the cracks. The direction of dislocation walls was perpendicular to the growth direction of the columnar crystal. The longer the annealing time was, the larger the length and width of the formed crack would be. A quantitative model of the crack growth was provided to calculate the length and width of the cracks at a given annealing time.

22 April 2017 in Materials
Verified
Journal Article
Open access
PDF file
Penghui LeiPenghui Lei
Penghui Lei
GRGuang Ran
Guang Ran
CLChenwei Liu
Chenwei Liu
CYChao Ye
Chao Ye
DLDong Lv
Dong Lv
JXJiangkun Xu
Jiangkun Xu
The microstructure evolution of Zr-1.1Nb-1.51Fe-0.26Cu-0.72Ni zirconium alloy, irradiated by 800 keV Kr2+ ions at 585 K using the IVEM-Tandem Facility at Argonne National Laboratory, was observed by in situ transmission electron microscopy. A number of β-Nb precipitates with a body-centered cubic (BCC) structure were distributed in the as-received zirconium alloy with micrometer-size grains. Kr2+ ion irradiation induced the growth of β-Nb precipitates, which could be attributed to the segregation of the dissolved niobium atoms in the zirconium lattice and the migration to the existing precipitates. The size of precipitates was increased with increasing Kr2+ ion fluence. During Kr2+ iron irradiation, the zirconium crystals without Nb precipitates tended to transform to the nanocrystals, which was not observed in the zirconium crystals with Nb nanoparticles. The existing Nb nanoparticles were the key factor that constrained the nanocrystallization of zirconium crystals. The thickness of the formed Zr-nanocrystal layer was about 300 nm, which was consistent with the depth of Kr2+ iron irradiation. The mechanism of the precipitate growth and the formation of zirconium nanocrystal was analyzed and discussed.

23 November 2017 in Nanomaterials
Verified
Journal Article
Open access
PDF file
CYChao Ye
Chao Ye
GRGuang Ran
Guang Ran
WZWei Zhou
Wei Zhou
YQYazhou Qu
Yazhou Qu
XYXin Yan
Xin Yan
NLNing Li
Ning Li
The nanocrystal 3C-SiC/ZrO2 bilayer films that could be used as the protective coatings of zirconium alloy fuel cladding were prepared on a single-crystal Si substrate. The corresponding nanocrystal 3C-SiC film and nanocrystal ZrO2 film were also dividedly synthesized. The microstructure of nanocrystal films was analyzed by grazing incidence X-ray diffraction (GIXRD) and cross-sectional transmission electron microscopy (TEM). The 3C-SiC film with less than 30 nm crystal size was synthesized by Plasma Enhanced Chemical Vapor Deposition (PECVD) and annealing. The corresponding formation mechanism of some impurities in SiC film was analyzed and discussed. An amorphous Zr layer about 600 nm in width was first deposited by magnetron sputtering and then oxidized to form a nanocrystal ZrO2 layer during the annealing process. The interface characteristics of 3C-SiC/ZrO2 bilayer films prepared by two different processes were obviously different. SiZr and SiO2 compounds were formed at the interface of 3C-SiC/ZrO2 bilayer films. A corrosion test of 3C-SiC/ZrO2 bilayer films was conducted to qualitatively analyze the surface corrosion resistance and the binding force of the interface.