Penghui Lei

Dr. Penghui Lei

School of Nuclear Science and Technology, Xi'an Jiaotong University, Xi'an 710049, China

Research Focus & Metrics

Academic Career Length

11Years (2016-Present)

(Calculated once Scilit publication data is synced: current year − year of first publication + 1)

Representative Publications

View All Publications
15 December 2017 in Metals
Verified
Journal Article
Open access
PDF file
JLJianxin Lin
Jianxin Lin
GRGuang Ran
Guang Ran
Penghui LeiPenghui Lei
Penghui Lei
CYChao Ye
Chao Ye
SHShilin Huang
Shilin Huang
NLNing Li
Ning Li
The microstructure of Al/B4C metal matrix composites (MMCs) used as neutron absorbers in both dry storage casks and wet storage pools of spent nuclear fuel was analyzed by SEM and TEM. A polishing method of a focused Ga+ ion beam was used to obtain an ideal sample surface with very low roughness, which was used to statistically analyze the distribution characteristics and size factor of B4C particles in the aluminum matrix. The area of B4C particles mainly ranged from 0 to 0.5 μm2, which was the proportion of 64.29%, 86.99% and 76.86% of total statistical results for the Al-15%B4C, Al-25%B4C and Al-30%B4C MMCs, respectively. The average area of B4C particles in the Al-15%B4C, Al-25%B4C and Al-30%B4C MMCs were about 1.396, 0.528 and 1.183 μm2, respectively. The nanoscale precipitates were analyzed by the element mappings in scanning transmission electron microscopy (STEM) mode and electron energy loss spectroscopy (EELS) mode, which included elliptic alloy precipitates with elemental Cu, Cr, Fe and Si, except for Al, and B4C nanoparticles with polygonal shape. The interface characteristics showed that the (021) crystal plane of B4C particle and (111) crystal plane of aluminum matrix grew together. The lattice misfit was about 1.68% for (111)Al//(021)B4C. The corrosion properties and corresponding mechanism of Al/B4C MMCs were investigated in an aqueous solution with 5000 ppm boric acid at 100 °C and atmospheric pressure, which showed that the mass increment rate was first decreased with increasing corrosion time and then increased.

28 December 2016 in Materials
Verified
Journal Article
Open access
PDF file
JHJinhua Huang
Jinhua Huang
GRGuang Ran
Guang Ran
JLJianxin Lin
Jianxin Lin
QSQiang Shen
Qiang Shen
Penghui LeiPenghui Lei
Penghui Lei
NLNing Li
Ning Li
The microstructural evolution of Dy2O3-TiO2 powder mixtures during ball milling and post-milled annealing was investigated using XRD, SEM, TEM, and DSC. At high ball-milling rotation speeds, the mixtures were fined, homogenized, nanocrystallized, and later completely amorphized, and the transformation of Dy2O3 from the cubic to the monoclinic crystal structure was observed. The amorphous transformation resulted from monoclinic Dy2O3, not from cubic Dy2O3. However, at low ball-milling rotation speeds, the mixtures were only fined and homogenized. An intermediate phase with a similar crystal structure to that of cubic Dy2TiO5 was detected in the amorphous mixtures annealed from 800 to 1000 °C, which was a metastable phase that transformed to orthorhombic Dy2TiO5 when the annealing temperature was above 1050 °C. However, at the same annealing temperatures, pyrochlore Dy2Ti2O7 initially formed and subsequently reacted with the remaining Dy2O3 to form orthorhombic Dy2TiO5 in the homogenous mixtures. The evolutionary mechanism of powder mixtures during ball milling and subsequent annealing was analyzed.

22 April 2017 in Materials
Verified
Journal Article
Open access
PDF file
Penghui LeiPenghui Lei
Penghui Lei
GRGuang Ran
Guang Ran
CLChenwei Liu
Chenwei Liu
CYChao Ye
Chao Ye
DLDong Lv
Dong Lv
JXJiangkun Xu
Jiangkun Xu
The microstructure evolution of Zr-1.1Nb-1.51Fe-0.26Cu-0.72Ni zirconium alloy, irradiated by 800 keV Kr2+ ions at 585 K using the IVEM-Tandem Facility at Argonne National Laboratory, was observed by in situ transmission electron microscopy. A number of β-Nb precipitates with a body-centered cubic (BCC) structure were distributed in the as-received zirconium alloy with micrometer-size grains. Kr2+ ion irradiation induced the growth of β-Nb precipitates, which could be attributed to the segregation of the dissolved niobium atoms in the zirconium lattice and the migration to the existing precipitates. The size of precipitates was increased with increasing Kr2+ ion fluence. During Kr2+ iron irradiation, the zirconium crystals without Nb precipitates tended to transform to the nanocrystals, which was not observed in the zirconium crystals with Nb nanoparticles. The existing Nb nanoparticles were the key factor that constrained the nanocrystallization of zirconium crystals. The thickness of the formed Zr-nanocrystal layer was about 300 nm, which was consistent with the depth of Kr2+ iron irradiation. The mechanism of the precipitate growth and the formation of zirconium nanocrystal was analyzed and discussed.

12 November 2016 in Nanomaterials
Verified
Journal Article
Open access
PDF file
SHShilin Huang
Shilin Huang
GRGuang Ran
Guang Ran
Penghui LeiPenghui Lei
Penghui Lei
SWShenghua Wu
Shenghua Wu
NCNanjun Chen
Nanjun Chen
NLNing Li
Ning Li
The self-assembly nanocone structures on the surface of polycrystalline tungsten were created by He+ ion irradiation and then annealing, and the resulting topography and morphology were characterized using atomic force microscopy and scanning electron microscopy. The cross-sectional samples of the self-assembly nanocones were prepared using an in situ–focused ion beam and then observed using transmission electron microscopy. The self-assembly nanocones were induced by the combined effect of He+ ion irradiation, the annealing process and the chromium impurity. The distribution characteristics, density and morphology of the nanocones exhibited a distinct difference relating to the crystal orientations. The highest density of the nanocones was observed on the grain surface with a (1 1 1) orientation, with the opposite for that with a (0 0 1) orientation and a medium value on the (1 0 1)-oriented grain. The size of the self-assembly nanocones increased with increasing the annealing time which met a power-law relationship. Irradiation-induced defects acted as the nucleation locations of the protrusions which attracted the migration of the tiny amount of chromium atoms. Under the action of temperature, the protrusions finally evolved into the nanocones.

22 October 2018 in Materials
Verified
Journal Article
Open access
PDF file
WSWenzhu Shen
Wenzhu Shen
CLChenwei Liu
Chenwei Liu
Penghui LeiPenghui Lei
Penghui Lei
GRGuang Ran
Guang Ran
Two types of Zr–0.8Sn–1Nb–0.3Fe Zr alloys were irradiated by krypton ions in the temperature range from 320 to 400 °C. The microstructure of the as-received alloys showed that the sizes of Zr crystals and (Zr, Nb)2Fe particles with face-centered cubic (FCC) structure increased from 3.9 μm to 6.0 μm and from 74.6 nm to 89.6 nm, respectively, after cold rolling and subsequent annealing. Kr+ irradiation-induced bubble formation in the Zr matrix was observed. The size of the gas bubbles increased with increasing ion fluence and irradiation temperature. An equation that related the bubble size, ion fluence, and temperature were established. Irradiation-induced amorphization of particles was observed and found to be related to the fabrication process and irradiation parameters. The particles in alloy #1 showed a higher irradiation tolerance than those in alloy #2. The threshold damage dose for the amorphization of particles in alloy #2 was 3.5 dpa at 320 °C and 4.9 dpa at 360 °C. The mechanisms for bubble growth and particle amorphization are also discussed.

13 November 2018 in Materials
Verified
Journal Article
Open access
PDF file
HSHongying Sun
Hongying Sun
Penghui LeiPenghui Lei
Penghui Lei
GRGuang Ran
Guang Ran
HWHui Wang
Hui Wang
JZJiyun Zheng
Jiyun Zheng
SQShui Qiu
Shui Qiu
As leading candidates of sheet steels for advanced nuclear reactors, three types of Ni–Mo–Cr high-strength low alloy (HSLA) steels named as CNST1, CNST2 and CNSS3 were irradiated by 400 keV Fe+ with peak fluence to 1.4 × 1014, 3.5 × 1014 and 7.0 × 1014 ions/cm2, respectively. The distribution and morphology of the defects induced by the sample preparation method and Fe+ irradiation dose were investigated by transmission electron microscopy (TEM) and positron-annihilation spectroscopy (PAS). TEM samples were prepared with two methods, i.e., a focused ion beam (FIB) technique and the electroplating and twin-jet electropolishing (ETE) method. Point defects and dislocation loops were observed in CNST1, CNST2 and CNSS3 samples prepared via FIB. On the other hand, samples prepared via the ETE method revealed that a smaller number of defects was observed in CNST1, CNST2 and almost no defects were observed in CNST3. It is indicated that artifact defects could be introduced by FIB preparation. The PAS S-W plots showed that the existence of two types of defects after ion implantation included small-scale defects such as vacancies, vacancy clusters, dislocation loops and large-sized defects. The S parameter of irradiated steels showed a clear saturation in PAS response with increasing Fe+ dose. At the same irradiation dose, higher values of the S-parameter were achieved in CNST1 and CNST2 samples when compared to that in CNSS3 samples. The mechanism and evolution behavior of irradiation-induced defects were analyzed and discussed.