The article dealt with the load-bearing capacity and durability of power line lattice towers designed from weathering steel. Attention was paid in particular to the bolted lap joints. The article evaluates the static and corrosion performance of bolted lap joints in long-term operating towers, and also presents and evaluates design measures that can be applied in the design of new lattice towers, or in the reconstruction of already operating structures. Power line lattice towers are the most extensive realization of weathering steel in the Czech Republic. On the basis of the inspections carried out to evaluate the working life of the transmission towers in operation, it can be stated that a sufficiently protective layer of corrosion products generally developed on the bearing elements of the transmission towers. However, the development of crevice corrosion at the bolted joints of the leg members is a significant problem. In this paper, the corrosion damage of bolted joints was evaluated considering two basic aspects: (1) the influence of crevice corrosion on the bearing capacity of the bolted joint was evaluated, using experimental testing and based on analytical and numerical calculations; (2) appropriate design measures applicable to the rehabilitation of developed crevice corrosion of in-service structures, or the elimination of crevice corrosion in newly designed lattice towers, was evaluated. Calculation analyses and destructive tests of bolted joints show that the development of corrosion products in the crevice does not have a significant effect on the bearing capacity of the joint, provided that there is no significant corrosion weakening of the structural elements, and bolts of class 8.8 or 10.9 are used. The results of the long-term experimental programme, and the experience from the rehabilitations carried out, show that, thanks to appropriate structural measures, specified in detail in the paper, the long-term reliable behaviour of the lattice towers structures is ensured.
Chloride ions are nowadays the main cause of the degradation of steel and reinforce concrete construction in the vicinity of the road. On the other hand, chloride ions, usually in the form of de-icing salts or brine, are very important for safe winter traffic on the roads. This creates a slightly schizophrenic situation where it is necessary to ensure safe traffic in the winter period and at the same time to affect the service life of the structure as little as possible. The effect of the roadway on chloride deposition is a long-studied, but still imprecisely understood, part of the effect of chloride ions on structures in the vicinity of the roadway. This paper discusses the experimental measurement of chloride deposition in the vicinity of the I/11 road in the Czech Republic by dry plate method, wet candle method and corrosion coupons. Statistical analysis of correlation and regression is performed on the results of measurements by wet candle and horizontal dry plate methods. The methods are interdependent. A detailed analysis of the surface and chemical properties of the corrosion products is performed on the corrosion coupons. Using the corrosion loss, the environmental category C2 is determined. Observation of the microclimate in the vicinity of the roads gives to engineers a basis for the correct design of structures around the roads. The conclusions of the experimental measurements are intended to help engineers to design a structure that is safe, serviceable and sufficiently resistant to chloride ions within its service life
In corrosion science, accurate determination of chloride ion deposition rates is critical to mitigating the environmental impact on structures. Traditional methods, such as the wet candle and dry plate methods (ISO 9225), are often inaccurate in capturing localized conditions and are also time-consuming and costly. The Bresle method, which measures soluble salts directly on metal surfaces, offers a more targeted approach. This article examines the Bresle method as an alternative for determining average monthly chloride ion deposition rates, including a regression analysis comparing the Bresle method with the wet candle method, and examines the long-term salinity of exposed surfaces in comparison with the additive approach to surface salinity. This paper hypothesizes that the Bresle method can be used as an alternative to the wet candle method. Linear regression analysis shows a strong correlation in chloride ion deposition rates compared to those measured by the wet candle method. However, cumulative measurements using long-term exposed coupons are unreliable due to inconsistent trends.
To date, many studies can be found in the literature attempting to explain the effects of temperature and humidity on the rate of corrosion processes. However, it is difficult to analyze the results of these studies and draw unambiguous conclusions due to the different test conditions as well as different electrochemical test methods for corrosion rates. Most of these studies concern concrete reinforced with ordinary steel. However, there is a lack of research and analysis conducted on prestressed elements. The purpose of this study was to evaluate the effect of temperature and humidity changes on the development of corrosion processes in prestressed concrete beams. Tests were performed both under conditions of increasing temperature and humidity, which were reproduced in a climatic chamber, as well as in an environment exposed to chloride ions. The process of migration of chloride ions into the concrete was accelerated by the application of an electric field. In addition, selected beams were subjected to prolonged loading to sustain the induced scratching. Corrosion rate tests were carried out using the non-destructive linear polarization method (LPR). Strength tests of the beams were also carried out, as well as displacement and deformation measurements using the Aramis system’s digital image correlation technique. The beams without chloride addition had a fairly stable low level of corrosion current density throughout the test period, indicating the passive state of the reinforcement, regardless of the environment in which they were placed and the additional loading. In an environment with a humidity of 30% and a temperature of 20 °C, the corrosion current density increment was much faster than for beams with chloride additives in an environment with a humidity of 90% and a temperature of 30 °C. A smaller increase in corrosion current density could be observed in beams that were scratched, compared to non-scratched beams. The results of the strength tests indicated that in beams subjected to accelerated migration of chloride ions, the deflection at scratching was significantly lower than in beams without chloride addition. Also in these beams, milder strains were registered on the surface of the elements at the time of scratching.
The present study investigates the influence of corrosion exposure on the fatigue behavior of S460NL high-strength structural steel, a material that is frequently utilized in offshore and civil engineering structures. Accelerated corrosion was simulated under controlled laboratory conditions for exposure periods of 3 days, 6 days, and 6 + 3 days, in addition to specimens subjected to natural atmospheric corrosion. To this end, fatigue tests were performed to obtain S–N curves, and the results were evaluated using Basquin's law and the probabilistic Castillo–Canteli model. The findings indicate that corrosion has a substantial impact on fatigue resistance. The endurance limit exhibited a decline from 214 MPa for the reference specimens to 176 MPa following three days of corrosion, 135 MPa after six days, and approximately 92 MPa after combined corrosion exposure, signifying a reduction of up to 57%. Fractographic observations revealed that corrosion pits act as stress concentrators, thereby promoting early crack initiation. A discernible correlation was identified between corrosion mass loss and normalized endurance limit. These findings highlight the importance of considering corrosion effects in fatigue life assessment and structural design of high-strength steel components.
The present study investigates the development of fatigue damage in welded S460 high-strength steel specimens subjected to different corrosion exposure conditions. Four surface conditions were considered: an uncorroded reference condition, 3-day exposure, 6-day exposure and combined 6+3-day exposure, hereafter referred to as 3D, 6D and 6+3D/9D, respectively. Fatigue tests were performed at a stress ratio of . Microscopic observations were carried out before and after fatigue testing using an Olympus DSX1000 digital microscope to evaluate surface degradation, crack/fracture localization and damage development in the welded region.The uncorroded reference condition showed fatigue damage that was predominantly localized in the welded region, thereby confirming the dominant role of weld geometry and the local notch effect. As the level of corrosion exposure increased, the surface condition changed progressively. The 3D condition exhibited limited early degradation, the 6D condition revealed more distinct surface defects, and the 6+3D/9D condition showed the most pronounced corrosion-product regions and pit-like surface damage. The fatigue results indicated a non-monotonic influence of corrosion exposure. The apparent improvement observed for the 3D and 6D conditions may be related to local modification of the weld-toe surface condition and partial mitigation of the original weld-induced notch effect.After fatigue testing, all representative specimens showed crack/fracture development near the weld toe and heat-affected zone (HAZ) vicinity. The findings indicate that fatigue damage was governed by the combined effect of weld-toe geometry, the visually distinguishable HAZ vicinity and corrosion-induced surface degradation.