Aluminum containing Mn+1AXn (MAX) phase materials have attracted increasing attention due to their corrosion resistance, a pronounced self-healing effect and promising diffusion barrier properties for hydrogen. We synthesized Ti2AlN coatings on ferritic steel substrates by physical vapor deposition of alternating Ti- and AlN-layers followed by thermal annealing. The microstructure developed a {0001}-texture with platelet-like shaped grains. To investigate the oxidation behavior, the samples were exposed to a temperature of 700 °C in a muffle furnace. Raman spectroscopy and X-ray photoelectron spectroscopy (XPS) depth profiles revealed the formation of oxide scales, which consisted mainly of dense and stable α-Al2O3. The oxide layer thickness increased with a time dependency of ~t1/4. Electron probe micro analysis (EPMA) scans revealed a diffusion of Al from the coating into the substrate. Steel membranes with as-deposited Ti2AlN and partially oxidized Ti2AlN coatings were used for permeation tests. The permeation of deuterium from the gas phase was measured in an ultra-high vacuum (UHV) permeation cell by mass spectrometry at temperatures of 30–400 °C. We obtained a permeation reduction factor (PRF) of 45 for a pure Ti2AlN coating and a PRF of ~3700 for the oxidized sample. Thus, protective coatings, which prevent hydrogen-induced corrosion, can be achieved by the proper design of Ti2AlN coatings with suitable oxide scale thicknesses.
Even though hard, low friction coatings such as diamond like carbon (DLC) would be beneficial for the performance and longevity of rubber seals, a crucial challenge remains. The elastic mismatch of rubber substrate and DLC coating prevents a fracture free coating application. In this work, a nature inspired approach is applied to render the stiff coating flexible and resilient to delamination at the same time by direct patterning. Rubber substrates were laser structured with tile patterns and subsequently DLC coated. Tensile and tribology tests were performed on structured and unstructured samples. Unstructured DLC coatings showed a crack pattern induced by the coating process, which was further fragmented by tensile stress. Coatings with tile patterns did not experience a further fragmentation under load. During continuous tribological loading, less heterogenous damage is produced for tile structured samples. The findings are ascribed to the relief of induced coating stress by the tile structure, meaning a more resilient coating.
Even though hard, low friction coatings such as diamond like carbon (DLC) would be beneficial for the per-formance and longevity of rubber seals, a crucial challenge – as graphically illustrated in Figure 1.a – remains. The elastic mismatch of rubber substrate and DLC coating prevents a fracture free coating application. In this work a nature inspired approach (Figure 1.b) is applied to render the stiff coating flexible and resilient to delamination at the same time by direct patterning. Rubber substrates were laser structured with tile patterns and subsequently DLC-coated. Tensile and tribology tests were performed on structured and unstructured samples. Unstructured DLC-coatings showed a crack pattern induced by the coating process, which was further fragmented by tensile stress. Coatings with tile patterns did not experience a further fragmentation under load. During continuous tribological loading, less heterogenous damage is produced for tile structured samples. The findings are ascribed to the relief of induced coating stress by the tile structure, meaning a more resilient coating.