The technological performance and environmental advantages of replacing sand by ornamental stone processing waste (OSPW) in the production of mortars for civil construction were studied. Technological properties associated with the standard consistency index, squeeze flow and bulk densities as well as the determination of water retention and calorimetry analysis were evaluated in the mortars’ fresh state, whereas capillarity tests as well as mechanical resistance by flexural and compression tests were determined in the hardened state for mortars incorporated with 10, 30 and 60 wt.% of OSPW substituting sand. Three different types of Portland Cements were considered in the incorporated mortars production. For these mortars environmental analysis, their corresponding life cycle assessment results were compared to that of conventional waste-free (0% OSPW) control mortar. It was found that the OPSW incorporation acts as nucleation sites favoring a hydration process, which culminates after 28 days of curing in the formation of more stable phases identified as hydrated calcium silicates by X-ray diffraction (XRD) amorphous halo. It was also revealed that both flexural and compression improved resistance for the incorporated mortars after 28 curing days. In particular, the calorimetry and XRD results explained the better mechanical resistance (12 MPa) of the 30 wt.% OSPW incorporated mortar, hardened with Portland Cement V, compared not only to the control, but also to the other incorporated mortars. As for the environmental analysis, the replacement of sand by OSPW contributed to the reduction in associated impacts in the categories of land use (−5%); freshwater eutrophication (−9%); marine eutrophication (−6%) and global warming (−5%).
12 September 2021 in Environmental Science and Pollution Research
Several polymeric compounds are obtained from synthetic organic solids containing petrochemical derivatives. Biochar fines are considered waste and an alternative bio-reinforcement in composite materials, potentially serving as a possible substitute for non-renewable polymers based on petrochemical derivatives. In this context, the present study focuses on analyzing the properties of biochar fines obtained from the pyrolysis of Eucalyptus sp. biomass, aiming to support the use of this waste in the fabrication of a composite using biochar as a bio-reinforcement. The biochar was produced through pyrolysis in a muffle furnace at a final temperature of 800 °C, with a heating rate of 5 °C min−1 and a residence time of 60 min. The characterization of the obtained fines involved proximate analysis, Brunauer–Emmett–Teller (BET) analysis, scanning electron microscopy (SEM), Fourier-Transform Infrared Spectroscopy (FTIR), thermogravimetric analysis (TGA), and X-ray diffraction (XRD). The results show that the material has a high fixed carbon content, high density, and good thermal resistance, making it stand out for use in composites.
6 June 2022 in Environmental Science and Pollution Research
Incorporating solid waste into polymeric matrices has proven effective in developing composites with enhanced mechanical and thermal properties. This study investigates a composite based on recycled high-density polyethylene (HDPE), reinforced with fine charcoal particles, assessing its thermal, microstructural, and density properties. Two processing methods (compression molding and extrusion) and four charcoal concentrations (0%, 5%, 10%, and 15 wt%) were evaluated. Thermal characterization was performed using thermogravimetric analysis (TGA) and Fourier transform infrared spectroscopy (FTIR). The microstructure was analyzed through scanning electron microscopy (SEM) and X-ray diffraction (XRD), while the density was determined via X-ray densitometry. SEM revealed increased porosity with charcoal addition. The thermal properties and crystallinity of the composites were not significantly affected by variations in the manufacturing method or charcoal concentration. FTIR analysis identified characteristic peaks, while TGA indicated mass loss between 400 and 500 °C, with a maximum decomposition temperature of 487 °C. XRD confirmed the semicrystalline structure typical of HDPE. Thus, incorporating charcoal residues can reduce the use of fossil-based materials while providing a sustainable application for industrial waste.
To ensure that metal recovery processes in electronic waste are truly sustainable from an industrial perspective, studies on the performance of such methodologies are necessary to verify the economic, environmental, social, and technological viabilities. The importance of conducting multicriteria and comparative investigations into the actual performances of methods used in the recovery of these materials is emphasized, considering trade-offs such as high efficiency in metal extraction balanced against intense consumption of energy and chemical reagents. The analytical hierarchy process, multicriteria decision support tool, and the life cycle assessment tool are proposed to be used in combination in this work to assess and contrast the environmental effects of two hydrometallurgical paths for the recuperation of copper in electronic circuit boards (PCBs). The results indicate that the sulfuric acid method had a copper solubilization efficiency of 90.05%, whereas the route employing the combination of ammonium sulfate and ammonia had an estimated copper solubilization efficacy of 49%. It was feasible to calculate the life cycle effects of the hydrometallurgical procedures connected to the copper recovery activities on the PCBs with regard to the LCA. Compared to the acidic leaching pathway, alkaline leaching was responsible for about 71% of the environmental damage discovered in the study, according to the AHP tool.