Al–Si eutectic alloys are industrially important; they play a significant role in the casting-manufacturing of most materials. The properties of the materials are governed by their microstructure, which can be tuned by adjusting the solidification process parameters. Herein, the effect of forced melt flow on the microstructure of an Al–Si eutectic alloy during unidirectional solidification was investigated experimentally. Al–12.6-wt%-Si alloy samples were solidified in a vertical Bridgman-type furnace equipped with a rotating magnetic inductor to induce flow in the melt. The samples were subjected to different magnetic induction conditions during the solidification experiments. The diameter of the samples was 8 mm, and their length was 120 mm. The eutectic alloy samples were solidified unidirectionally at a growth rate of v ≈ 0.1 mm/s and a temperature gradient of G ≈ 6 K/mm. The inter-lamellar distances (λ), lengths, and orientation angles of the Si lamellae were investigated using new measurement methods. The experimental results reveal that applying the rotating magnetic field (RMF) during the solidification has a distinct effect on the microstructure of Al–Si eutectic alloys. Indeed, the RMF refines the eutectic structure, reduces the interlamellar distances, and increases the diversity of the Si lamella angle’s orientations. However, the successive stirring process has a negligible effect on the lengths and angles of Si lamellae.
Using magnetic stirring during solidification provides a good opportunity to control the microstructure of alloys, thus controlling their physical properties. However, magnetic stirring is often accompanied by a change in local concentrations, and new structures form which could harm the physical properties. This research paper investigated the effect of forced melt flow by a rotating magnetic field (RMF) on the macrostructure of an Al-Si eutectic alloy. To serve this purpose, Al-12.6 wt% Si alloy samples were solidified in a vertical Bridgman-type furnace equipped with a rotating magnetic inductor to induce the flow in the melt. The diameter and length of the sample are 8 mm and 120 mm, respectively. The solidification parameters are a temperature gradient (G) of 6 K/m, and the solid/liquid front velocity (v) of 0.1 mm/s. These samples were divided into parts during the solidification process, where some of these parts are solidified under the effect of RMF stirring while others are solidified without stirring. The structure obtained after solidification showed a distinct impact of stirring by RMF; new phases have been solidified which were not originally present in the structure before stirring. Besides the eutectic structure, the new phases are the primary aluminum and the primary silicon. The Si concentration and the volume fraction of each phase were measured using Energy-Dispersive Spectroscope (EDS)and new image processing techniques. The experimental results reveal that applying the RMF during the solidification has a distinct effect on the macrostructure of Al-Si eutectic alloys. Indeed, the RMF provokes macro-segregation, reduces the amount of eutectic structure, and changes the sample’s Si concentration distribution.