In this work, we refer to the fraction of hydrides and vinyl groups consumed in cross‐linking reaction as a variation of the properties of poly(dimethylsiloxane) (PDMS) with varying the formulation of a curing agent from 3.2 wt % to 50 wt %. Young's modulus, density, and refractive indices of PDMS were observed to have a maxima at a formulation of about 10 wt % of cross linker. The intensity of the Raman band for the SiH stretching mode in cross‐linker is almost zero if the cross‐linking agent is less than 10 wt %, but it is linearly increasing with increasing the content of cross‐linker. The dependence of the elastic modulus on the formulation could be explained in terms of the fraction of cross‐linked network. The analytical framework proposed in this work could be used for optimizing the formulation of PDMS and hence its properties can be tailored for specific applications.
1 October 1997 in The Journal of Physical Chemistry B
Cyanobacteriochromes (CBCRs) are a subfamily of phytochrome photoreceptors found exclusively in photosynthetic cyanobacteria. Four CBCRs containing a second Cys in the insert region (insert-Cys) have been identified from the nonheterocystous cyanobacterium Microcoleus B353 (Mbr3854g4 and Mbl3738g2) and the nitrogen fixing, heterocystous cyanobacterium Nostoc punctiforme (NpF2164g3 and NpR1597g2). These insert-Cys CBCRs can sense light in the near-UV to orange range, but key residues responsible for tuning their colour sensitivity have not been reported. In the present study, near-UV/Green (UG) photosensors Mbr3854g4 (UG1) and Mbl3738g2 (UG2) were chosen for further spectroscopic analysis of their spectral sensitivity and tuning. Consistent with most dual-Cys CBCRs, both UGs formed a second thioether linkage to the phycocyanobilin (PCB) chromophore via the insert-Cys. This bond is subject to breakage and relinkage during forward and reverse photoconversions. Variations in residues equivalent to Phe that are in close contact with the PCB chromophore D-ring in canonical red/green CBCRs are responsible for tuning the light absorption peaks of both dark and photoproducts. This is the first time these key residues that govern light absorption in insert-Cys family CBCRs have been identified and characterised.
Nonlinear multiphoton absorption induced by focusing near infrared (NIR) femtosecond (fs) laser pulses into a transparent cornea allows surgery on neovascular structures with minimal collateral damage. In this report, we introduce an fs laser-based microsurgery for selective treatment of rat corneal neovascularizations (in vivo). Contiguous tissue effects are achieved by scanning a focused laser pulse below the corneal surface with a fluence range of 2.2–8.6 J/cm2. The minimal visible laser lesion (MVL) threshold determined over the corneal neovascular structures was found to be 4.3 J/cm2. Histological and optical coherence tomography examinations of the anterior segment after laser irradiations show localized degeneration of neovascular structures without any unexpected change in adjacent tissues. Furthermore, an approximately 30 % reduction in corneal neovascularizations was observed after 5 days of fs laser exposure. The femtosecond laser is thus a promising tool for minimally invasive intrastromal surgery with the aid of a significantly smaller and more deterministic photodisruptive energy threshold for the interaction between the fs laser pulse and corneal neovascular structures.
We have investigated the effect of the dynamics of crater size on the poly(dimethylsiloxane) (PDMS) surface morphology in fs-laser micro-processing. PDMS surface was processed with varying both inter-pulse interval and inter-spot distance between successive laser pulses. With keeping the interval of 5 ms crater shape is round even if the spot is overlapped in space. But decreasing the interval to 0.02 ms the shape of the crater is no longer round. Decreasing the inter-distance between the craters results in roughened surface morphology even at time intervals of 5 ms. Temporal dependence of single-shot fs-laser induced crater size was measured as a function of time delay. Within 0.1 ms after pulse irradiation with a fluence of 4.8 J/cm2 on PDMS surface the crater size has reached to its maximum values and then decreased with a time constant of about 0.3 ms. The surface morphology after fs-laser pulse irradiation is strongly dependent on not only inter-spot distance between successive laser pulse but also their inter-pulse intervals. By proposing a theoretical model on their dynamic features, we will try to explain the current observation in quantitatively.
Coherent anti-Stokes Raman scattering (CARS) microscopy is demonstrated to be a promising optical method for the characterization of polymer films with film thickness varying between 180 nm to 4300 nm. In case of PMMA films with a thickness of few hundreds of nanometers, the observed CARS signal was mainly associated with the interference effect of large nonresonant CARS field from glass substrate and the weak resonant field of PMMA. The dependence of resonant CARS intensity of PMMA film on film thickness is in good agreement with the theoretical prediction on a CARS field. The current work offers potential possibilities of noninvasive thickness measurement of polymeric thin film of thickness less than 180 nm by multiplex CARS microscopy without depth-profiling.