A substantial contribution of the stresses that arise inside the Plasma-Facing Components (PFCs) when a heat load is applied is caused by the mismatch of the Coefficient of Thermal Expansion (CTE) between the armor, usually made of tungsten (W), and the heat sink. A potential way to reduce such contribution to the secondary stresses is the use of an interlayer made with a Functionally Graded Material (FGM), to be interposed between the two sub-components. By tailoring the W concentration in the volume of the FGM, one can engineer the CTE in such a way that the thermal stresses are reduced inside the PFC. To minimize and, theoretically, reduce to zero the stresses due to the CTE mismatch, the FGM should ensure kinematic continuity between the armor and the heat sink, in a configuration where they deform into exactly the shape they would assume if they were detached from each other. We will show how this condition occurs when the mean thermal strain of each sub-component is the same. This work provides a methodology to determine the thickness and the spatial concentration function of the FGM able to ensure the necessary kinematic continuity between the two sub-components subjected to a generic temperature field monotonously varying in the thickness, while remaining stress-free itself. A method for the stratification of such ideal FGM is also presented. Additionally, it will be shown that the bending of the PFC, if allowed by the kinematic boundary conditions, does not permit, at least generally, the coupling of the expansion of the armor and of the heat sink. As an example of our methodology, a study case of the thermomechanical design of a steel-based PFC with an engineered W/steel FGM interlayer is presented. In such an exercise, we show that our procedure of engineering a FGM interlayer is able to reduce the linearized secondary stress of more than 24% in the most critical section of the heat sink, satisfying all the design criteria.
3 June 2024 in IEEE Transactions on Plasma Science
The Divertor Tokamak Test (DTT) facility is a fusion device under construction in Italy. The mission of DTT is to test alternative divertor concepts under integrated physics and technological conditions that can reliably be extrapolated to DEMO. Due to the plasma core characteristics with relevant edge and scrape-off layer (SOL) parameters and a wall entirely in tungsten (W), DTT will provide an extensive set of information useful to select the most appropriate strategy for the power exhaust in DEMO. Several divertors, which may differ in design or/and technologies or/and poloidal profile, will be tested during the life of the machine. The first divertor to be installed will have to accommodate a multitude of strike points, located at various positions according to the different magnetic configurations, which will be tested in the first operational phases of the machine with the aim to identify the most promising. The first divertor will not test innovative technological solutions but will mainly take advantage of the technologies already qualified for the ITER divertor production. Thus, the entire divertor plasma-facing surface is designed to be used as targets: it will be made of W monoblocks joined on CuCrZr pipes (plasma-facing units, PFUs) similar to the ITER targets. With the purpose to increase the flexibility in operational scenarios by maximizing the allowable thermal load for the PFUs, the possibility of using monoblocks with a plasma side reduced thickness was investigated. By reducing the thickness of the armor, it is possible to limit plastic deformation of the monoblock and to preserve the characteristics of the plasma-facing surface during the component lifetime. A thickness between 3 and 4 mm is compatible both the erosion estimates in the DTT divertor area and the manufacturing constraints and therefore proposed for the DTT PFUs. Several mock-ups based on monoblock design were in the past tested under thermal fatigue, confirming the reliability of the monoblock design and the manufacturing processes, but with larger armor thicknesses (6–8 mm). The experimental verification of the monoblock performance with the proposed reduced thickness has been verified in the GLADIS facility at IPP Garching with a thermal load of 20 MW/m $^{2}$ applied for 1000 cycles of 10 s. The results showed the absence of plastic deformation and negligible increase in surface roughness.
The optimal configuration choice between positive triangularity (PT) and negative triangularity (NT) tokamaks for fusion power plants hinges on navigating different operational constraints rather than achieving specific plasma performance metrics. This study presents a systematic comparison using constrained multi-objective optimization with the integrated FUsion Synthesis Engine (FUSE) framework. Over 200 000 integrated design evaluations were performed exploring the trade-offs between capital cost minimization and operational reliability (maximizing q95 ) while satisfying engineering constraints including 250 ± 50 MW net electric power, tritium breeding ratio 1.1, power exhaust limits and an hour flattop time. Both configurations achieve similar cost-performance Pareto fronts through contrasting design philosophies. PT, while demonstrating resilience to pedestal degradation (compensating for up to 40% reduction), are constrained to larger machines ( R0 6.5 m) by the narrow operational window between L–H threshold requirements and the research-established power exhaust limit ( 15 MW m −1 ). This forces optimization through comparatively reduced magnetic field (∼8 T). NT configurations exploit their freedom from these constraints to access compact, high-field designs ( m, B0 12 T), creating natural synergy with advancing HTS technology. Sensitivity analyses reveal that PT’s economic viability depends critically on uncertainties in L–H threshold scaling and power handling limits. Notably, a 50% variation in either could eliminate viable designs or enable access to the compact design space. These results suggest configuration selection should be risk-informed: PT offers the lowest-cost path when operational constraints can be confidently predicted, while NT is robust to large variations in constraints and physics uncertainties.
11 April 2024 in IEEE Transactions on Plasma Science
The main mission of the divertor tokamak test (DTT) facility is to study advanced solutions for the power exhaust issue in view of a fusion power plant. In this respect, a significant amount of heat is expected to be absorbed by the first wall (FW) during operation. Therefore, the DTT FW is designed to be an actively water-cooled system. A proper hydraulic model is needed for the development of a cooling architecture of the system able to fulfill the requirements of operational safety under thermal loads and compliance with the DTT plant specifications. The present study aims to address this challenge, offering practical inputs for further optimization. Based on the existing conceptual design, the cooling circuits have been setup inside the plasma-facing components (PFCs). In this phase, empirical equations and hydraulic simulations have been adopted to investigate the hydraulic behavior of the modules that make up the FW and to evaluate the main design parameters, namely, velocity and pressure drops in the cooling channels. The outcome of such analysis demonstrated that the current design of the FW system complies with the imposed requirements. Moreover, operating flexibility has been demonstrated by identifying a proper range of the mass flow rate for each subsystem. Therefore, the models implemented in this study and the obtained findings prove to be suitable to support the next activities of engineering design of the FW.
17 April 2024 in IEEE Transactions on Plasma Science
The divertor tokamak test (DTT) facility is currently in the design stage and in the initial phase of construction at the research center ENEA Frascati. The DTT facility aims at searching integrated solutions for the power exhaust issue maintaining plasma performances compatible with future fusion devices. For this reason, the first DTT divertor was designed to accommodate different magnetic configurations: in particular other than single null (SN), the compatibility with X-divertor (XD) and negative triangularity (NT) with different leg lengths was ensured. To accommodate the strike point positions of the different magnetic equilibria, all plasma facing surfaces (i.e., inner and outer vertical targets, as well as the dome) have to be entirely made of tungsten (W) monoblocks. At the same time, to leave more space to the divertor legs, it was decided to design a dome with a flat shape. These two factors along with the armor with W monoblock and the flat shape have required finding ad hoc technological solutions for the plasma facing units (PFUs) of the dome with the need of a research and qualification phase. Above all, a W flat tiles (FTs) design was required at the inner dome end, where the copper cooling pipes turn by 90 $^{\circ}$ . The FT segment covers only a small length of the PFU ( $\sim$ 40 mm), and the goal is to join both monoblock and FT segments to the pipe in a single manufacturing process. The technique used is the hot radial pressing (HRP), which has been developed in ENEA and qualified for the manufacturing of the ITER inner vertical target.
This contribution presents a didactic overview of the sustainability of nuclear fusion as a source for electricity production. A comparison with traditional means of electricity generation will be carried out, especially regarding waste production. Particular attention will be focused on the lifetime of components in a fusion reactor, since this engineering parameter determines directly the environmental and economic sustainability. Finally, the impact of heat exhaust components, which is the field of expertise of the authors, on waste production will be assessed and the most active research activities aimed to enhance the performance and lifetime of these components will be summarized.