In focus of this report are the mechanisms of formation, propagation, and interaction of growth defects in heteroepitaxial diamond films along with their impact on the optical emission properties of N- and Si-vacancy (NV and SiV) color centers. Here, we analyze and discuss the properties of incoherent grain boundaries (IGBs) and extended defects in a nitrogen- and boron-doped heterodiamond nucleated and grown on Ir(001) via bias-enhanced nucleation and chemical vapor deposition techniques. We show that the low-angle IGBs alter the structural and optical emission properties of NV and SiV complexes by subduing NV emission and supporting the formation of interstitial Si-vacancy complexes dominating in the faulted IGB regions. We also demonstrate that the IGB-confined threading dislocations are responsible for the vertical transport and incorporation of Si impurities in thick layers, leading to an enhanced SiV emission from the IGBs.
31 May 2019 in The Journal of Physical Chemistry A
For the wafer-scale fabrication of diamond devices, the growth of diamond substrates by heteroepitaxial chemical vapor deposition is the most promising option currently available. However, the transfer of growth and also structuring processes from small homoepitaxial to larger heteroepitaxial samples is not straightforward and requires adaptation. In this study, we present an approach for the fabrication of functional microstructures including pyramids and mesas as well as more complex structures with hollow centers. The associated methods were previously demonstrated by homoepitaxial growth and are now evaluated on heteroepitaxially grown diamond films. After optimizing the growth procedures to ensure a sufficient quality of the bare diamond substrates, precursor structures for overgrowth were fabricated by e-beam lithography and plasma etching. In the overgrowth of nanopillars, a truncated pyramidal shape was achieved. The characterization with scanning electron microscopy revealed the growth of higher-index facets. Nevertheless, photoluminescence spectroscopy reveals localized doping on the sides of the microstructures. In addition, optically detected magnetic resonance reaches a contrast of 6% of one preferred nitrogen vacancy orientation per facet and a transverse relaxation time T2∗ of 96 ns.
15 November 2018 in The Journal of Chemical Physics
Temperature Programmed Desorption (TPD) spectroscopy was used to determine the binding energies of polycyclic aromatic hydrocarbons CnHm (22 ≤ n ≤ 60) with highly oriented pyrolytic graphite. These energies were then used to estimate the dispersive graphite interlayer cohesion by means of a refined extrapolation method proposed by Björk et al. This yields a cohesion energy of 44.0 ± 3.8 meV per carbon atom. We discuss some limits of the TPD-based approach and contrast our values with previous determinations of the interlayer cohesion energy of graphite.