Selective laser melting (SLM) technology is ushering in a new era of advanced industrial production of metal components. It is of great importance to understand the relationship between the surface features and electrochemical properties of manufactured parts. This work studied the influence of surface orientation on the corrosion resistance of 316L stainless-steel (SS) components manufactured with SLM. The corrosion resistance of the samples was measured using linear polarization resistance (LPR) and electromechanical noise (EN) techniques under three different environments, H2O, 3.5 wt.% NaCl, and 20% H2SO4, analyzing the horizontal (XY) and vertical (XZ) planes. The microstructure and morphology of the samples were obtained by optical (OM) and scanning electron microscopy (SEM). The obtained microstructure showed the grains growing up from the fusion line to the melt pool center and, via SEM-EDS, the presence of irregular and spherical pores was observed. The highest corrosion rate was identified in the H2SO4 solution in the XZ plane with 2.4 × 10−2 mm/year and the XY plane with 1.31 × 10−3 mm/year. The EN technique along with the skewness factor were used to determine the type of corrosion that the material developed. Localized corrosion was observed in the NaCl electrolyte, for the XY and XZ planes (−1.65 and −0.012 skewness factors, respectively), attacking mainly the subgrains of the microstructure and, in some cases, the pores, caused by Cl ions. H2O and H2SO4 solutions presented a uniform corrosion mechanism for the two observed orientations. The morphology identified by SEM was correlated with the results obtained from the electrochemical techniques.
The present work presents the analysis of corrosion behavior of 304 and 316 stainless steels in comparison with the AISI 1018 steel, as reinforcement in concrete specimens made with partial replacement of CPC 30R-RS by Sugar Cane Bagasse Ash (SCBA) and Silica Fume (SF), the specimens were exposed to a 3.5% solution of Na2SO4, as an aggressive medium. The electrochemical techniques employed in the present study were the half-cell potential, (ASTM C-876-15) and Linear Polarization Resistance LPR (ASTM G59). The Ecorr values after more than 100 days of exposure indicate for the three steels present corrosion uncertainty, however the values of Icorr of stainless steel 304 and 316 indicate 5 times more resistant corrosion than AISI 1018 steel, presenting the concrete made with SCBA, the best performance against corrosion when exposed to sulfates.
The present investigation was conducted to study the oxidation kinetics of nickel-based superalloy 263, used in the manufacture of rings for aircraft engines. For carrying out this study, we first conducted microstructural characterization of the pieces using the techniques of optical microscopy, scanning electronic microscopy, and X-ray diffraction. Subsequently, using the thermogravimetric analysis, the kinetic oxidation of the metal was performed in a temperature range between 700 and 1000°C, using atmospheres of O2. The results of the micrographs show the formation of a protective oxide film on the surface of the material in different oxidizing agents. Finally, it was found that the kinetics of high-temperature oxidation of the superalloy C-263 obeys the parabolic rate law.