The present study presents a numerical prediction of residual stresses (RS) using the single-pass tungsten inert gas (TIG) welding process for stainless steel plates and the two-pass TIG welding process for stainless steel pipes. The effect of heat exchange between welding material and the environment was studied. The work consists of two parts: The first one is based on the determination of the existence of residual stresses numerically using Cast3M software, which has been validated by literature results. The second part addresses the means envisaged to attenuate the amplitudes of these residual stresses by practical methods. Two parameters with significant influence on the residual stresses have been chosen: the welding bead thickness and the torch displacement speed. The finite element model used has been validated experimentally, and the results obtained for the residual stresses have been compared with those given by the numerical study. The results obtained were found to be in agreement with references results. In addition, the microstructural analysis of different areas after welding of the solder joint (base metal, heat-affected zone and solder zone) was carried out using optical microscopy analysis.
This work investigates the effect of the notch on fatigue behavior by combining two methods: the extended finite element method (XFEM) and the averaged strain energy density (ASED) method, which considers the combined action of bending and shear loading. The ASED method has already been proven accurate for assessing the failure of components in the presence of sharp and blunt notches, and several results are available in the literature for different materials. These results were compared with those obtained from the experimental tests reported here. The main purpose of this study was twofold: The first part is an experimental study of fatigue in rotary bending of specimens weakened by U and V notches made of polymethyl-methacrylate (PMMA) material. Two values for the radius were used for the U-notches (0.2 and 2 mm) and two angles for the V-notches (20° and 140°). The second part of the study consisted of performing several simulation tests using the Cast3m software for different angles and radii. The local approach based on the mean value of the ASED acted over a finite-sized volume surrounding the highly stressed regions. The maximum principal stress located at the notch edge defined the center of the control volume. If
25 March 2022 in Fracture and Structural Integrity
This study has used the strain energy density (SED) approach to evaluate the stress intensity factor (SIF) of cracked cruciform welded joints in Hardox 450 steel. A microstructural analysis was made of Hardox 450 steel which is composed of refined and tempered low carbon martensite. The obtained results of simulation will be compared with those provided by J-integral methode for different enriched zones and contours based on the extended finite element method (XFEM) coupled with the level set technique (LST). Crack initiation and propagation under cyclic loading have been adopted for the modeling of cruciform welded joints.
15 November 2016 in Journal of Adhesion Science and Technology
The present work is aimed to investigate the effect of notch root radius ρ and angle of specimen on the critical effective T-stress. A notched plate made of molybdenum alloy TZM is considered and subjected to a tensile loading. In brittle materials, the tools derived from linear elastic fracture mechanics are applicable and the analysis was made according to a local approach defined by the volumetric method. Different values of notch root radius (ρ = 0.5, 1, 1.5, 2 mm) and angle ( = 0°, 15°, 30° and 45°) have been selected to conduct an analysis of the critical effective T-stress and the distribution of T-stress at the notch tip in brittle fracture. The effective T-stress Teff has been estimated as the average value of the T-stress distribution in the region ahead of the notch tip at the effective distance Xeff. The obtained results showed that the variation of radius affects strongly the critical effective T-stress, while the variation of angle gives a very small change in values of critical effective T-stress.