The effect of long-term ageing (1000, 2000, and 3000 h) at 475 °C on mechanical properties, microstructure, and substructure of CUSTOM 465® maraging stainless steel was studied. The additional precipitation of nanometric particles of η-Ni3Ti phase in partly recovered lath martensite and decomposition of the BCC solid solution accompanied by the formation of nanometric Cr-rich α’particles were identified. The fraction of reverted austenite in the final microstructure gradually increased with time of ageing at 475 °C. Ageing resulted in a gradual slight decline (up to 10%) in yield strength, ultimate tensile strength, and hardness. On the other hand, for all ageing, dwells ductility and impact energy values remained almost unchanged. The reason for this phenomenon lies in the gradual increase in the fraction of reverted austenite during long-term ageing at 475 °C and at the same time in the sluggish kinetics of microstructural changes in lath martensite. No susceptibility to 475 °C embrittlement was proved.
It is not realistic to optimize the roll pass design of profile rolling mills, which typically roll hundreds of profiles, using physical modelling or operational rolling. The use of reliable models of microstructure evolution is preferable here. Based on the mathematical equations describing the microstructure evolution during hot rolling, a modified microstructure evolution model was presented that better accounts for the influence of strain-induced precipitation (SIP) on the kinetics of static recrystallization. The time required for half of the structure to soften, t0.5, by static recrystallization was calculated separately for both situations in which strain-induced precipitation occurred or did not occur. On this basis, the resulting model was more sensitive to the description of grain coarsening in the high-rolling-temperature region, which is a consequence of the rapid progress of static recrystallization and the larger interpass times during rolling on cross-country and continuous mills. The modified model was verified using a plain strain compression test (PSCT) simulation of rolling a 100-mm-diameter round bar performed on the Hydrawedge II hot deformation simulator (HDS-20). Four variants of simulations were performed, differing in the rolling temperature in the last four passes. For comparison with the outputs of the modified model, an analysis of the austenite grain size after rolling was performed using optical metallography. For indirect comparison with the model outputs, the SIP initiation time was determined based on the NbX precipitate size distribution obtained by TEM. Using the PSCT and the outputs from the modified microstructure evolution model, it was found that during conventional rolling, strain-induced precipitation occurs after the last pass and thus does not affect the austenite grain size. By lowering the rolling temperature, it was possible to reduce the grain size by up to 56 μm, while increasing the mean flow stress by a maximum of 74%. The resulting grain size for all four modes was consistent with the operating results.
In austenitic steels, the tetragonal Z-phase (NbCrN) has frequently been credited with beneficial strengthening effects during dislocation creep. In the modified Z-phase, niobium is partially substituted by vanadium. The basic objective of this contribution is a detailed characterization of the modified Z-phase in vanadium bearing austenitic AISI 316LN+Nb+V and HR3C steels. Experimental activities were focused on crystallography, thermodynamic and dimensional stability, kinetics of precipitation (TTP diagram) and solvus temperature of the modified Z-phase in the steels examined. Thermodynamic modelling was used for prediction of stable minor phases and solvus temperature of the modified Z-phase. Kinetics of precipitation of the (Nb,V)CrN phase in the AISI 316LN+Nb+V steel was experimentally investigated in the temperature interval of 550–1250 °C. The kinetics of precipitation of the modified Z-phase in austenitic matrix was fast. Results of diffraction studies on particles of the modified Z-phase confirmed the existence of the tetragonal unit cell already after short-term annealing. The solvus temperature of the modified Z-phase in austenitic steels was determined to be lower than that for the NbCrN phase. The decrease in the solvus temperature is dependent on the vanadium content in austenitic steels. Both thermodynamic calculations and experimental results proved that the thermodynamical stability of the modified Z-phase in austenite was high. More data are needed for evaluation of long-term dimensional stability of the (Nb,V)CrN phase in austenitic steels at temperatures for their engineering applications.
1 November 2019 in IOP Conference Series: Materials Science and Engineering
This contribution deals with the formation and decomposition of Widmanstätten austenite during solidification of the thin belt-casted strips made of a grain oriented electrical steel (GOES). Solidification of liquid steel started with the formation of δ-ferrite. Cooling in the δ + γ phase field resulted in the formation of a small fraction of Widmanstätten austenite by displacive mechanism accompanied by carbon partition. Widmanstätten austenite laths formed flat low energy interface facets along ferrite grain boundaries. In order to minimize the interfacial energy, ferrite grain boundaries in the vicinity of flat austenite/ferrite facets migrated. It resulted in the formation of either straight or zig-zag ferrite boundaries. Intensive precipitation of sulphides along ferrite/austenite interfaces made it possible to study the early stages of austenite decomposition at the end of the δ + γ phase field. Complex sulphides containing chromium, manganese, iron and copper were identified as the Cr2CuS4 phase. Decomposition of austenite started with the formation of epitaxial ferrite. This was accompanied by further partitioning of carbon into remaining austenite. The growth of epitaxial ferrite into the flat ferrite/austenite interface facets along ferrite grain boundaries resulted in a wavy shape of these boundaries. Finally, remaining carbon rich austenite transformed either to pearlite or plate martensite.