This work covers the effectiveness of the White tea extract as a green corrosion inhibitor and is correlated to the strength and stability bonding between the phenolic molecule and the Fe atoms in mild steel and how this interaction can be studied by altering the concentration and temperature. White tea has received considerable attention due to its capability as a corrosion inhibitor and has been extensively studied using electrochemical techniques. However, accurate and systematic functional group identification and surface modification have been missing. Our study sought to demonstrate the quantitative measurement of electrochemical impedance spectroscopy (EIS) complemented by the FTIR (Fourier transform infrared spectroscopy), Total Phenolic Test, and Raman Spectroscopy. The SEM (Scanning Electronic Microscope)/EDX (Energy-Dispersive X-Ray Spectroscopy), and AFM (Atomic Force Microscope) were used to study the surface modification. The EIS results show that the optimum inhibition efficiency was 96 % in a solution of 80 ppm at 60 °C. Acetone 70 % was used to extract White tea and gives 14.17±0.25 % phenolic compound. Spectroscopic studies show -OH, Aromatic C=C, C=O and C-O-C become major contributors in the adsorption process and are found on the surface of metals as corrosion protection. Meanwhile, the thermodynamic calculation shows the White tea was adsorbed chemically. The nearness of R2 to 1 shows the adsorption agrees with the Langmuir adsorption isotherm. Eventually, the surface modification revealed that phenol molecules are responsible to reduce the corrosion rate at 16.38×10-3 mpy. Our results are expected to provide a guideline for future research in White tea as a green corrosion inhibitor
Ferronickel slag is a by-product of nickel smelting that provides an abundant silica source. Based on data, every ton of nickel production is equal to eight tons of ferronickel slag production, increasing without any recycling process. It is essential to create an end-to-end process for nickel production and its by-products because this would be a problem in the future and is relevant for many industrialized countries. This study describes a strategy to process ferronickel slag to produce silica. A pyrometallurgy–hydrometallurgy process and ferronickel slag were used to increase the silica content. The process was conducted through alkali fusion; the ferronickel slag was mixed with sodium carbonate at a temperature of 1000 °C for an hour and continued via leaching, precipitation, and cleaning processes. The leaching process was conducted with four concentrations (4 M, 6 M, 8 M, and 10 M) of sodium hydroxide and three different leaching durations (2 h, 4 h, and 6 h). Using hydrochloric acid (HCl) at pH 2 and deionized (DI) water cleaning, the precipitation process was adopted to synthesize a silica powder with the lowest agglomeration and enhance its purity. Characterization was carried out using X-ray Diffraction (XRD), Scanning Electron Microscopy–Energy-Dispersive Emission (SEM-EDS), X-ray Fluorescence (XRF), and Inductively Coupled Plasma–Optical Emission Spectroscopy (ICP-OES). This study highlighted silica characteristics that indicate high recovery by 85% through alkali fusion, HCl leaching, precipitation, and deionized water cleaning.
30 April 2020 in Eastern-European Journal of Enterprise Technologies
One of the industries that play a role in supporting the development of the country is the oil and gas industry. In addition, this industry has an influence on the country’s economy, so it must be operated as efficiently as possible so as not to produce substantial costs and not have a significant impact on the country’s economy. The oil and gas industry is equipped with good supporting equipment that plays an important role in the success of the production process. The most important equipment for the continuity of production is the pipe. Generally, this pipe is made of mild steel and the material commonly used for pipes in the oil and gas industry is API 5L. Corrosion is one of the challenges found in pipes in the oil and gas industry. This is due to aggressive ions such as Cl– and also the fluid contained in the pipe. The aggressive ions that exist can cause corrosion in the form of pitting corrosion. Corrosion that occurs in pipes in the oil and gas industry must be addressed as efficiently as possible with effective results. Inhibitors are one solution that can provide effective results in reducing corrosion rates. Corrosion rate can be reduced by 99 % or more if the concentration of the inhibitor is appropriately added. Generally, inhibitors that are often used are inorganic inhibitors, where these inhibitors contain chemical compounds that are harmful to the environment and health. So, currently there are many developed environmentally friendly inhibitors, namely inhibitors produced from plants and fruits. Environmentally friendly inhibitors do not have an impact on environmental pollution because the material from these inhibitors has organic properties. Until now, there have been many studies on environmentally friendly inhibitors carried out on API 5L steel. However, there have been no studies on inhibitors obtained from Areca Flower extract as environmentally friendly inhibitors. Thus, this study was conducted in order to determine the effect of adding environmentally friendly inhibitors on the corrosion behavior of API 5L steel pipes in aggressive environments, namely HCl media. Areca flower extract has been investigated as a green corrosion inhibitor on API 5L Grade B in 1 M HCl acidic solution using Linear polarization and Electrochemical Impedance Spectroscopy (EIS). Additions of 4 ml, 8 ml, 12 ml, 16 ml, and 20 ml of corrosion inhibitors increase the efficiency of the inhibitors. Optimum inhibition efficiency occurs with the addition at a concentration of 20 ml is 96.6 % on Electrochemical Impedance Spectroscopy (EIS) testing. Polyphenolic and flavonoid compounds contained in the areca flower inhibit corrosion by physical adsorption, to form a monolayer which can inhibit corrosion. Adsorption occurs spontaneously in accordance with Langmuir isothermal adsorption. The polarization showed that the areca flower extract acts through mixed-type inhibition. The value of the free energy of –7.026 kJ/mol of adsorption indicated that the adsorption of inhibitor molecules was typical of physical adsorption
8 August 2022 in ASCE-ASME Journal of Risk and Uncertainty in Engineering Systems, Part B. Mechanical Engineering
The work reports the systematic approach to the study of artificial intelligence (AI) in addressing the complexity of inline inspection (ILI) data management to forecast the risk in natural gas pipelines. A recent conventional standard may not be sufficient to address the variation data of corrosion defects and inherent human subjectivity. Such methodology undermines the accuracy assessment confidence and is ineffective in reducing inspection costs. In this work, a combination of unsupervised and supervised machine learning and deep learning has profoundly accelerated the probability of failure (PoF) assessment and analysis. K-means clustering and Gaussian mixture models show direct relevance between the corrosion depth and corrosion rate, while the overlapping PoF value is scattered in three clusters. Logistic regression, support vector machine, k-nearest neighbors, and ensemble classifiers of AdaBoost, random forest, and gradient boosting are constructed using particular features, labels, and hyperparameters. The algorithm correctly predicted the score of PoF from 4790 instances and confirmed the 25% metal loss at a location of 13.399 m. The artificial neural network (ANN) is designed with various layers (input, hidden, and output) architecture. It is optimized using an activation function to predict that 74% of the pipeline's anomalies that classified at low-medium and medium-high risk. Furthermore, it provides a quick and precise prediction about the external defects at 13.1 m and requires the personnel to conduct wrapping composite. This work can be used as a standard guideline for risk assessment based on ILI and applies to industry and academia.
30 April 2023 in Eastern-European Journal of Enterprise Technologies
In the oil and gas industry, maintaining the integrity of production equipment is critical to ensuring the industry’s sustainability. Failure to maintain the integrity of production equipment can result in financial losses for the business. The management of production equipment nearing the end of its design life faces an increasing cost of Inspection, Maintenance, and Repair (IMR). As a result, a strategy to improve the efficiency of IMR is essential. Recent IMR management practices include predictive Risk-Based Inspection (RBI), which is more efficient than Time-Based Inspection (TBI). The research intends to evaluate the 28-year-old subsea sales gas pipeline using API 581 standard quantitative methodology by utilizing the Inline Inspection (ILI). Specifically, the study focuses on measuring the Probability and Consequence Failure of inspected pipelines. The inspection interval is determined based on the minimum allowable thickness. The risk calculation indicates that 12 pipeline segments are at a medium risk level (3 segments, 1D and 1E, and 2C). The remaining nine segments remain at lower risk (1C). Based on the result, segment nine is accepted as the highest PoF value of 1.04E-4 failures per year due to high depletion values due to the higher CoF value at the leak location. The calculation of the inspection interval indicates that the forthcoming Inspection will be due 20 years post the previous assessment. Another method using the Estimated Repair Factor (ERF) thickness limit approach produces the same results. However, assessment using ASME B31.8S provides different results of 10 years intervals when using the same ILI inspection method. This work can be used as a standard guideline to assess the risk of pipelines over a decade in service
The study reports the development of a liquid smoke solution of rice husk ash (RHA) as a green corrosion inhibitor in NH4Cl solution in approaching corrosion protection for refinery facilities. The recent utilization of RHA has a partial solution to address the possible chemical to form a filming layer to disconnect bare metal and their environment. This work prepared the RHA solution by condensing the RHA vapor before adding it to various concentrations. The corrosion test of potentiodynamic and electrochemicals intends to discover the inhibitor's corrosion resistance before examining the electronic transition corresponding to the contribution of several functional groups using Ultraviolet Visible (UV–Vis) and Fourier-Transform Infrared Spectroscopy (FTIR). Surface evaluation intends to unveil the nature of the corrosion by utilizing the Scanning Electronic and Atomic Force Microscope. The corrosion test result shows the depression of corrosion rate to 0.120 mmpy with high efficiency beyond 96 % in the addition of 7.5 ppm RHA inhibitor. The greater Nyquist semicircle diameter at high concentrations increases the adsorption of the RHA on the surface of C1018. The electronic transition of n–π* and π –π* shows an extensive contribution of C <!-- PBM data was replaced with SVG by xgml2pxml: 000000000000 000000000000 000000000000 111111111111 000000000000 111111111111 000000000000 000000000000 000000000000 --> Created by potrace 1.16, written by Peter Selinger 2001-2019 C, C O, and –OH based on the UV–Vis and FTIR test. The formation of a complex compound of Fe-(NH4Cl-RHA)n blocks the corrosion active sites to reduce the corrosion. This study paves the way for using RHA as an organic compound under NH4Cl conditions, such as in a refinery process facility.