In order to determine the effect of defect size on the pipeline fracture performance of girth welds in oil and gas pipelines, ABAQUS was used to simulate the fracture responses of X80 pipelines with girth weld defects under internal pressure and bending moment conditions based on damage mechanics. In particular, the length and depth of defects were parametrically studied; the defect depth range was 20–80% of the wall thickness, and the circumferential length range of the defects was 5–20% of the pipeline circumference. The results show that, under the combined action of internal pressure and bending moment, the defect depth was more associated with adverse effects than the circumferential length of the defect. The failure load did not linearly decrease as the size of the defect increased, but when the depth of the defect reached a certain value, the failure load suddenly decreased.
In the field of oil and gas transportation, X80 pipelines are susceptible to localized plastic deformation caused by mechanical impact or geological activity. This leads to the formation of dents and the introduction of pre-strain, thereby affecting the structural integrity and fatigue life. This study systematically investigates the influence mechanism of pre-strain on the high-cycle fatigue performance of dented regions in X80 steel. Fatigue tests conducted across pre-strain levels of 1%, 2%, and 3% revealed that the induced plastic strain significantly degrades fatigue performance. Under constant stress amplitude, fatigue life decreases markedly with increasing pre-strain, a trend driven by the accumulation of micro-damage. Furthermore, a parametric P-S-N curve model that incorporates both pre-plastic strain and reliability was developed, providing a basis for quantitatively assessing the impact of pre-strain. By combining finite element analysis with the Smith-Watson-Topper (SWT) critical plane method, it was predicted that fatigue cracks in unconstrained dent primarily initiate at the dent periphery, with the critical plane orientation perpendicular to the circumferential direction, which aligns well with field observations. Parametric analysis indicates that the maximum operating pressure is the dominant factor affecting the fatigue life of the dented pipelines. This research elucidates the material-level fatigue failure characteristics of dented X80 pipelines and provides theoretical insights for life prediction and engineering protection.
This study systematically investigates the degradation and failure prediction of pipeline materials in sulfur-containing environments, with a particular focus on X52 pipeline steel exposed to high-sulfur environments. Through uniaxial tensile tests to assess mechanical properties, it was found that despite surface corrosion and a reduction in overall structural load-bearing capacity, the intrinsic mechanical properties of X52 steel did not exhibit significant degradation and remained within standard ranges. The Johnson–Cook constitutive model was developed to accurately capture the material’s plastic behavior. Subsequently, a genetic algorithm-optimized backpropagation (GABP) neural network was employed to predict the failure pressure of defective pipelines and the corrosion rate in acidic environments, with prediction errors controlled within 5%. By integrating the GABP model with NACE standard methods, a framework for predicting the remaining service life for in-service pipelines operating in sour environments was established. This method provides a novel and reliable approach for pipeline integrity assessment, demonstrating significantly higher accuracy than traditional empirical models and finite element analysis.
L360QS pipeline steel, due to its high toughness, high strength, resistance to sulfide stress cracking, and resistance to hydrogen-induced cracking, is increasingly being used in pipeline network construction. Its fracture behavior is a critical factor for safe operation in mountainous steep-slope environments, but it has not yet been widely studied. Therefore, this paper conducts extensive experiments on the ductile fracture of L360QS pipeline steel. The tests employed standard tensile, notched tensile, shear, and compression specimens, covering a stress triaxiality range from approximately −0.33 to 0.92. The study combined Ling’s iterative method to establish an elastoplastic constitutive model considering post-necking behavior, and incorporated it into finite element models to extract the average stress triaxiality and equivalent plastic strain at the moment of fracture initiation for each type of specimen. Based on the extracted data, a piecewise ductile fracture model was established: a simplified Johnson–Cook criterion is used in the high triaxiality range, while an empirical function is used to describe fracture behavior in the medium, low, and negative triaxiality ranges. The model was validated using a train–test split approach, predicting fracture displacements for an independent test set of specimens. The results showed all prediction errors were within 5%, demonstrating the model’s high accuracy. Furthermore, a Spearman correlation analysis quantified the influence of geometric factors, revealing that notch curvature has the strongest monotonic relationship in controlling average stress triaxiality and fracture strain. The fracture model established in this paper can accurately predict the fracture behavior of L360QS pipeline steel and provides a reliable basis for failure prediction and safety assessment under complex service conditions (such as mountainous steep slopes).