Blending a certain proportion of basalt fiber into concrete improves the toughness of concrete, which prevents cracking and avoids the brittle behaviors. In this paper, the compressive, tensile, and flexural tests of concrete with different basalt fiber contents were carried out. Then the test phenomena, failure modes, and mechanical properties were compared and analyzed to derive the relationship between the basalt fiber contents and mechanical properties. The toughness and crack resistance performance of basalt fiber reinforced concrete were evaluated by the fracture energy, advanced toughness parameters, and characteristic length proposed by Hillerborg. The correlation coefficient of basalt fiber was introduced to establish the calculation formula for mechanical properties of basalt fiber reinforced concrete. The results indicated that basalt fiber significantly improved the toughness and crack resistance performance of concrete. The enhancing effect of the basalt fiber on the compressive strength of concrete is lower than that of tensile strength and flexural strength. Moreover, the improvement effect was the highest with the basalt fiber content was 0.3% and 0.4%.
In order to determine the effect of defect size on the pipeline fracture performance of girth welds in oil and gas pipelines, ABAQUS was used to simulate the fracture responses of X80 pipelines with girth weld defects under internal pressure and bending moment conditions based on damage mechanics. In particular, the length and depth of defects were parametrically studied; the defect depth range was 20–80% of the wall thickness, and the circumferential length range of the defects was 5–20% of the pipeline circumference. The results show that, under the combined action of internal pressure and bending moment, the defect depth was more associated with adverse effects than the circumferential length of the defect. The failure load did not linearly decrease as the size of the defect increased, but when the depth of the defect reached a certain value, the failure load suddenly decreased.
Welding is the main method for oil/gas steel pipeline connection, and a large number of girth welds are a weak part of the pipeline. Under extremely complex loads, a steel pipeline undergoes significant plastic deformations and eventually leads to pipeline fracture. A damage mechanics model is a promising approach, capable of describing material fracture problems according to the stress states of the materials. In this study, an uncoupled fracture 2D model with a function of fracture strain and stress triaxiality, two uncoupled 3D fracture models, a consider the effect of Lode parameter stress-modified critical strain (LSMCS) model, and an extended Rice–Tracey (ERT) criterion were applied to X80 pipeline girth welds. Comprehensive experimental research was conducted on different notched specimens, covering a wide range of stress states, and the corresponding finite element models were established. A phenomenon-based hybrid numerical–experimental calibration method was also applied to determine the fracture parameter for these three models, and the stress triaxiality of the influence law of the tensile strength was analyzed. The results showed that the proposed fracture criterion could better characterize the ductile fracture behaviors of the girth welds of the X80 pipeline; however, the prediction accuracy of the 3D fracture model was higher than that of the 2D fracture model. The functional relationship between the tensile strength and stress triaxiality of the X80 pipeline girth welds satisfied the distribution form of the quadratic function and increased monotonically. The research results can be used to predict the fracture of X80 pipeline girth welds under various complex loads.
6 September 2022 in Journal of Composite Materials
Using pre-stressed carbon fibre reinforced polymer/plastic (CFRP) to strengthen bridge structures is currently considered a promising technology and the durability of the structure is closely related to the material property. CFRP have good corrosion resistance, but they also experience different degrees of swelling, corrosion and hydrolysis in water immersion environments. Stress accelerates this effect and leads to deterioration of the mechanical properties of the materials. This work aims to investigate the durability of CFRP grids under water, wet-dry cycles of seawater, seawater immersion and 0% fu ( fu is the ultimate tensile strength of the tested CFRP grids and it is constant stress in this paper), 30% fu, 60% fu coupled environments.Test aging time at room temperature (25°C) of 30, 60, 120, 180, 270, 360 days. The results indicate that the surface of epoxy resin is smooth at the initial moment by comparing of scanning electron microscope (SEM) image. With the increase of deterioration degree with aging time, the cavities and cracks appeared in the matrix. The epoxy resin content between the fibers decreased, and the adhesion force decreased. When the aging time is short, the tensile damage section of CFRP grid is flaky and the matrix is tightly bonded with the fiber. The later damage is mainly blow-up damage, which the fracture section is typical filiform. After CFRP grids aged for 360 days, the tensile strength decreased by 6.2%, 10.2%, 10.9% in the water, seawater solution and seawater wet-dry cycle environments. The tensile strength decreased by 10.2%, 12.3% and 20.2% under the coupling of seawater and different stress levels. A semi-empirical model of durability is proposed to provide a good reference value for the durability prediction of FRP materials.
Fiber-reinforced polymer (FRP) bars are one of the promising alternatives for steel bars used in concrete structures under corrosion or non-magnetic environments due to the unique physical properties of FRP materials. When compared with steel bars, FRP bars are difficult to be spliced in field application due to their anisotropy and low shear and compressive strengths. In view of this, the paper presents a new non-metallic connection system (i.e., resin-filled glass fiber-reinforced polymer (GFRP) pipe connection system) for the butt splicing of FRP bars. With the proposed connection system and a simplified trilinear interfacial bond-slip model, a set of design formulas were derived based on the requirement that the proposed connection system should provide a load transfer capacity beyond the tensile capacity of the spliced FRP bars (i.e., to fulfill the high tensile strength of FRP materials). Besides, considering the fabrication error-induced load transfer capacity reduction of the connection system in field application, a correction factor was introduced in the paper to compensate for the reduced load transfer capacity by increasing the FRP bar anchorage length. At last, to estimate the effectiveness of the proposed connection system and the derived design formulas, nine specimens were fabricated with a kind of commercially available basalt fiber-reinforced polymer (BFRP) bars and the designed connection system and tested under unidirectional tension to study their tensile performance. With the comparison between the tested and theoretical results, the effectiveness of the proposed connection system and the derived design formulas are verified.
Peeling failure at the interface is one of the main failure modes for CFRP (Carbon Fiber-Reinforced Polymer)-reinforced steel structures. However, there are very few reported studies on the bond-slip relationship at the CFRP-steel interface. A series of simple shear tests were carried out in the present paper. The influence of the fiber fabric’s width and thickness, the surface roughness of the steel sheet, and the thickness of the adhesive layer on the bonding performance of the CFRP fabric to steel interface was considered. The interface constitutive model and bonding strength model were further established under multiple factors. The results show that with the decrease of the surface roughness, the interface’ ultimate peeling load increases gradually, and the failure has a tendency to develop from a glue-steel interface to a glue-CFRP interface. The test pieces that were subjected to sand blasting obtained the peak value of the ultimate peeling load. This indicates that sand blasting can effectively enhance the interface bonding strength. The theoretical values obtained via the interface prediction model are consistent with the experimental values. This proves that the newly developed interface prediction model can effectively predict the local bonding slip and bonding strength of the interface.