A new advanced dual-phase (DP) steel characterized by ferrite and bainite presence in equal fractions has been studied within this paper. The anisotropy change of this steel was assessed as a progressively more severe cold rolling process was introduced. Specifically, tensile tests were used to build a strain-hardening curve, which describes the evolution of this DP steel’s mechanical properties as the thinning level increases from 20 to 70% with 10% step increments. As expected, the cold rolling process increases mechanical properties, profoundly altering the material’s microstructure, which was assessed in depth using Electron Backscatter Diffraction (EBSD) analysis coupled with the Kernel Average Misorientation (KAM) maps. At the same time, the process strongly modifies the material planar anisotropy. Microstructural and mechanical assessment and the Kocks–Mecking model applied to this steel evidenced that a 50% strain hardening makes the DP steel isotropic. The material retains or resumes anisotropic behavior for a lower or higher degree of deformation. Furthermore, the paper evaluated the forming limit of this DP steel and introduced geometric limitations to testing the thin steel plates’ mechanical properties.
This work aims to investigate the processability of René 80 via laser powder–bed fusion (L-PBF). René 80 is a poorly weldable Ni-superalloy, currently processed via investment casting to fabricate turbine blades working at an operating temperature of about 850 °C. The L-PBF parameters optimization aims to increase part integrity and enhance processing repeatability. This part was tackled by creating a complete design of experiments (DOE) in which laser power, scan speed and hatching distance were varied accordingly. Optimizing the abovementioned parameters minimized the crack density and pore area fraction. Hence, five parameter sets leading to a crack density lower than 100 µm/mm2 and a pore fraction between 0.045% and 0.085% were selected. Furthermore, the intra-print repeatability was studied by producing three specimens’ repetitions for each optimal set of parameters in the same build. The porosity value obtained was constant among repetitions, and the crack density (around 75 µm/mm2) had a slight standard deviation. The third step of the research assessed the inter-prints repeatability by producing a replica of the five selected parameter sets in a different build and by comparing the results with those studied previously. According to this latter study, the porosity fraction (ca. 0.06%) was constant in intra- and inter-print conditions. Conversely, crack density was lower than 100 µm/mm2 only in three sets of parameters, regardless of the intra- or inter-build cross-check. Finally, the best parameter set was chosen, emphasizing the average flaw fraction (least possible value) and repeatability. Once the optimal densification of the samples was achieved, the alloy’s microstructural features were also investigated.
2 November 2024 in Journal of Materials Research and Technology
Rapid L-PBF Printing of IN718 Coupled with HIP-Quench: A Faster Approach to Combine Manufacturing and Heat Treatment in a Nickel-Based Alloy Emilio Bassini,