Microscale silicon particles in lithium-ion battery anodes undergo large volume changes during (de)lithiation, resulting in particle pulverization and surface area increase concomitant with a continuous growth of the solid-electrolyte-interphase. One approach to overcome these phenomena is to operate the silicon anode under capacity-limited conditions (i.e., with partial capacity utilization). Since crystalline silicon is irreversibly transformed into amorphous phases upon lithiation, the purpose of the partial capacity utilization is to maintain a crystalline phase and thus prevent particle disintegration. Here, we investigate the amorphization process of micro-sized silicon particles in a silicon-rich anode (70 wt% silicon) over extended charge/discharge cycling in half-cells with a lithium reference electrode, varying the lower cutoff potential of the Si electrode. While the capacity of Si electrodes after formation remain constant for lithiation cutoffs of ≥170 mV vs Li+/Li, their capacity continuously increases over cycling for cutoffs of <170 mV vs Li+/Li, implying an ongoing amorphization of the crystalline phase. To quantify the ratio of the amorphous phase fraction over cycling, we employed an in-situ XRD method, utilizing the copper reflex of the current collector as internal standard. This allowed to determine the extent of amorphization over the course of cycling depending on the lithiation potentials.
21 November 2019 in Journal of the Electrochemical Society
In this paper, the concept of partial lithiation of silicon microparticles in anodes for lithium ion batteries is presented. These particles are accessible on an industrial scale and processing to anodes is possible using standard equipment in aqueous conditions. Compared to state-of-the-art high capacity graphite anodes, the initial volumetric anode capacity is increased by more than 40% in case the silicon capacity is utilized by around 30%, even with only light calendering of the anode. Partial utilization of the capacity that is offered by the available silicon leads to more stable cycling with accessible cycle numbers of up to 250 full cycles against NMC-622.
1 August 2021 in Journal of the Electrochemical Society
Due to its high capacity, rate capability and attractive cost position, the partial lithiation of silicon microparticles in anodes for Lithium Ion Batteries (LIB) is a material concept worth considering. Limitations in cycling stability and volume change currently limit its deployment to niche applications with moderate cycle life requirements and thus prevent a broader market introduction. The present study discusses the failure mechanism of LIB cells based on partially lithiated silicon dominant anodes. The loss of active lithium is reflected in a comparatively strong capacity decrease, especially at low cut-off voltages. The developed electrochemical methodology enables to differentiate between various loss contributions, such as lithium loss by electronic particle decoupling or particle isolation, trapping of mobile lithium and immobilization of lithium in the solid electrolyte interphase (SEI). The study identifies the continuous formation of SEI as the main failure mechanism, while particle decoupling, in addition, mainly contributes when operating at low discharge voltages. Approaches to increasing the cell performance consequently lie in the optimization of the electronic particle connection and in the development of improved electrolyte systems and/or pre-lithiation strategies to improve the cycle stability of silicon-based LIB cells.
Organosilanes play an important role in organic synthesis as well as in a variety of further areas, ranging from life science to transportation. Especially, the electrochemical access has become increasingly important in the past years and developed into an essential topic due to new conceptual approaches and mediated reaction control. With the commercial availability of high‐quality electrochemical equipment, the technical requirements for electro‐conversion are at hand to a wide audience. This results in the need for a concise survey of electrochemical silane transformation, appropriate for novices as well as experts alike. This review provides an overview of the most relevant work in this field, identifies common obstacles in working with chlorosilanes and hydrosilanes and bridges the gap between known techniques and novel methods with respect to their electrochemical conversion. The historical development is outlined with reference to the various cathodic as well as anodic conversions and should encourage to expand the research field of electrochemical silane transformation.
Using only parts of the maximum capacity of silicon microparticles in a lithium-ion battery (LIB) anode represents a promising material concept. The high capacity, better rate capability compared with graphite and accessibility on an industrial scale, as well as its attractive cost make microsilicon an ideal choice for the next generation anode material. However, currently the cycle life of LIBs using silicon particles in the anode is limited due to drastic volume change of Si during lithiation and delithiation. Continuous formation of a solid electrolyte interphase (SEI) and the associated lithium loss are the main failure mechanisms, while particle decoupling from the conductive network plays a role mainly during operation at low discharge voltages. The present study discusses approaches on the material- and cell-level to enhance cycle performance of partially lithiated silicon microparticle-based full cells by addressing the previously described failure mechanisms. Reducing the surface area of the silicon particles and coating their surface with carbon to improve the electronic contact, as well as prelithiation to compensate for lithium losses have proven to be the most promising approaches. The advantageous combination of these routes resulted in a significant increase in cycling stability exceeding 600 cycles with 80% capacity retention at an initial capacity of about 1000 mAh g−1 at anode level, compared to only about 250 cycles for the non-optimized full cell.
2 September 2024 in Journal of the Electrochemical Society
Due to its high specific capacity, silicon is one of the most promising anode materials for next-generation lithium-ion batteries. However, its large volumetric changes upon (de)lithiation of ∼300% lead to a rupture/re-formation of the solid-electrolyte interphase (SEI) upon cycling, resulting in continuous electrolyte consumption and irreversible loss of lithium. Therefore, it is crucial to use electrolyte systems that form a more stable SEI that can withstand large volume changes. Here, we investigate lithium nitrate (LiNO3) and lithium nitrite (LiNO2) as electrolyte additives. Linear scan voltammetry on carbon black working electrodes in a half-cell configuration with LiNO3-containing 1 M LiPF6 in EC/DEC (1/2 v/v) revealed a two-step reduction mechanism, whereby the first reduction peak could be attributed to the conversion of LiNO3 to LiNO2, while X-ray photoelectron spectroscopy on harvested electrodes suggests the formation of Li3N during the second reduction peak. On-line electrochemical mass spectrometry (OEMS) on carbon black electrodes showed that N2O gas is evolved upon the reduction of LiNO3- and LiNO2-containing electrolytes but that the gassing associated with EC reduction is significantly reduced. Furthermore, OEMS and voltammetry were used to examine the redox chemistry of LiNO2 additive. Finally, LiNO3 and LiNO2 additives significantly improved the cycle-life of Si||NCM622 full-cells.