Ti555211 titanium alloy is subjected to plastic deformation in the dual-phase (α + β phase) zone and single-phase (β phase) zone at various deformation temperatures and strain rates. High-temperature constitutive equations of the alloy in the dual-phase zone and single-phase zone are established in order to describe deformation behavior of the alloy in the different phase zones. By comparing the constitutive equation of the alloy in the dual-phase zone with that of the alloy in the single-phase zone, the deformation activation energy of the former was found to be higher than that of the latter. It is obvious that the deformation activation energy of α phase is obviously greater than that of β phase. Furthermore, the microstructural evolution of the alloy is different in the dual-phase zone and single-phase zone. When the alloy was subjected to plastic deformation in the dual-phase zone, the size of the grains in the β phase increased with the decreasing strain rate. When the alloy was subjected to plastic deformation in the single-phase zone, the size of the grains in the β phase considerably increased with the increasing deformation temperature. In particular, in the microstructures of the alloy subjected to plastic deformation in the single-phase region, the elongated grains can be observed at higher strain rates. Furthermore, it is more difficult for the alloy to induce plastic deformation in the dual-phase region than in the single-phase region.
9 January 2024 in IEEE Transactions on Applied Superconductivity
NbTi superconducting Wire has the advantage of excellent processing characteristics, stable superconducting properties, and low cost. It has been widely used for low magnetic fields of <9 T. To increase the stability and reduce the cost of superconducting magnets, it is necessary to improve the critical current density at high magnetic fields (≥9 T) of the NbTi superconducting wire. Therefore, this research focuses on the processing procedure and obtain samples with the higher Jc (4.2 K, 9 T) of 738 A/mm 2 . In addition, in this article, the microstructure of two typical samples with different Jc (4.2 K) at magnetic fields of 4 T and 9 T is analyzed. It is shown that the critical current density at high magnetic fields (≥9 T) needs the larger width and less area ratio of α-Ti phase.
The formation and evolution of adiabatic shear behaviors, as well as the corresponding mechanical properties of a near-Ti-6Al-3Nb-2Zr-1Mo (Ti-6321) alloy during dynamic compression process, were systematically investigated by the split Hopkinson pressure bar (SHPB) compression tests in this paper. Ti-6321 samples containing three types of microstructures, i.e., equiaxed microstructure, duplex microstructure and Widmanstätten microstructure, were prepared to investigate the relationship between microstructures and dynamic mechanical behaviors under different strain rates in a range from 1000 s−1 to 3000 s−1. It was found by the dynamic strain–stress relation that the Ti-6321 alloys containing equiaxed microstructure, duplex microstructure and Widmanstätten microstructure all exhibited a strong strain-hardening effect. The samples containing equiaxed microstructure exhibited a larger flow stress than samples containing duplex microstructure and Widmanstätten microstructure. The adiabatic shearing behaviors in Ti-6321 alloy are significantly influenced by different types of microstructures. The formation of adiabatic shearing bands occurs in equiaxed microstructure when the strain rate is increased to 2000 s−1. The adiabatic shear bands are formed in duplex microstructure when the strain rate reaches 3000 s−1. However, the initiation of adiabatic shear bands is found in Widmanstätten microstructure under the strain rate of 1000 s−1. The Widmanstätten microstructure shows a larger sensitivity to adiabatic shearing than the equiaxed microstructure and duplex microstructure samples.
7 November 2023 in Journal of Materials Research and Technology
In the present work, the localized features of adiabatic shear bands (ASBs) of our recently designed damage tolerance α+β dual-phase Ti alloy are investigated by the integration of electron backscattering diffraction and experimental and theoretical Schmid factor analysis. At the strain rate of 1.8 × 104 s−1 induced by a split Hopkinson pressure bar, the shear stress reaches a maximum of 1951 MPa with the shear strain of 1.27. It is found that the α+β dual-phase colony structures mediate the extensive plastic deformations along α/β phase boundaries, contributing to the formations of ASBs, microvoids, and cracks, and resulting in stable and unstable softening behaviors. Moreover, the dynamic recrystallization yields the dispersion of a great amount of fine α grains along the shearing paths and in the ASBs, promoting the softening and shear localization. On the contrary, low-angle grain boundaries present good resistance to the formation of cracks and the thermal softening, while the non-basal slipping dramatically contributes to the strain hardening, supporting the promising approaches to fabricate the advanced damage tolerance dual-phase Ti alloy.
In this study, high strain rate tension tests are conducted to determine and compare the dynamic mechanical behaviors and deformation mechanisms of different phase composition α-β metastable β-Ti alloys using a split Hopkinson tension bar. Two typical bimodal equiaxed αp + β and lamellar αs + β Ti-45551 alloy microstructures are formed through different hot working and thermal processing for investigating the effect of phase composition or microstructure on mechanical properties and strain rate sensitivity. It is demonstrated that dislocation nucleation and motion in the α/β phase and dislocation tangle or pile up at the α/β interface are typical deformation modes in both of the typical dual-phase Ti alloys at quasi-static loading conditions. Under dynamic loading, both the strength and ductility show a clearly positive strain rate dependence, which is directly related to dislocation activation in the α + β Ti-45551 alloy. Based on microstructure characterizations, it is shown that deformation twinning starts to become a major deformation mechanism in equiaxed αp + β microstructures under dynamic loading conditions. However, deformation twins are not favored in the lamellar αs + β Ti-45551 alloy due to its nano phase size. Finally, the mechanical behaviors and strain rate sensitivity are strongly dependent on the phase composition of metastable β-Ti alloys.