Surface treatments help to protect the built heritage against damage (environmental, accidental, etc.), reducing repair and restitution costs and increasing the useful life of building materials. The use of nanomaterials is currently the most important field of research in surface treatment technology for the preservation of building materials and, more specifically, to improve their durability and prevent their deterioration, extending their useful life. This paper studies the influence of a graphene oxide (GO) suspension as a surface treatment on the properties of concrete. The results indicate that, at best, surface treatment with GO can decrease both the water absorption and capillary absorption of concrete by about 15 %. The increase in the amount of GO deposited as a surface treatment leads to a further reduction in concrete water absorption. It is shown that, at best, GO coating also reduces water penetration at low and high pressures by approximately 20 % and 60 %, respectively. In addition, scanning electron microscopy analysis shows that GO surface treatment facilitates the hydration process and densifies the concrete microstructure. A simple aqueous suspension of GO is revealed as a tool with a high potential to protect concrete surfaces in a fast and cost-effective way, thanks to the easy application by spraying and the small amount of material needed to obtain great results.
26 January 2023 in Construction and Building Materials
Improving the protection of concrete by applying graphene oxide (GO) as a surface treatment has become the objective of the present study. This study focuses on performing a statistical analysis to study different levels of GO application as an exterior coating, thus observing the effectiveness of the coating and the optimization of the treatment material for concrete protection. Four tests were performed to define concrete durability, such as pressurized water penetration, capillary absorption, freeze-thaw resistance and carbonation resistance. The results showed an increase in concrete durability with any level of GO application on the surface, considering that the optimum amount of application for water impermeability and freeze-thaw resistance is 26.2 µg/cm2, since it was possible to reduce pressurized water penetration by 45%, capillary water absorption by 57% and freeze-thaw detachment by 25%. However, the optimum application rate for carbonation resistance is 52.4 µg/cm2, reducing carbonation by almost 60%. In conclusion, if the concrete is going to be exposed to less aggressive environments, the application of a mild surface coating of GO is sufficient for its protection, and if the concrete is going to be exposed to more aggressive environments, it is necessary to increase the amount of GO. The performance of GO as a coating significantly increased the degree of protection of the concrete, increasing its service life and proving to be a promising treatment for concrete surface protection.
24 February 2024 in Journal of Building Engineering