To deeply analyze the difference between styrene–butadiene–styrene (SBS)-modified asphalt and base asphalt in ultraviolet (UV) aging performance, an atomic force microscope was used to carry out an accurate analysis of the bee structural characteristic parameters of two kinds of asphalt experiencing different UV aging time duration. With the advantages of the Levenberg–Marquardt (LM) algorithm and universal global optimization (UGO) algorithm, the relationship between the microscopic characteristic value and the performance index of asphalt under UV aging was constructed. The results show that the physical parameters of the bee structure of asphalt are closely related to the macroscopic properties of asphalt materials. Because the number of bee structures of SBS-modified asphalt is significantly more than that of base asphalt, and in the process of UV aging, the absolute height and area of the bee structure fluctuate less, and the adhesion force fluctuates with aging time. The decreasing trend makes SBS-modified asphalt significantly better than base asphalt in anti-UV aging performance. Under different UV aging time durations, the penetration and aging index (AI) of the two kinds of asphalt showed an excellent linear relationship with the microscopic indexes measured by atomic force microscope (AFM). Through the nonlinear optimization algorithm, the prediction equations of the morphology height and adhesion force of the two kinds of asphalt under different aging stages were successfully derived. The research results can provide theoretical support for the optimization and improvement of the UV aging performance of SBS-modified asphalt.
This study investigates the evolution laws and prediction models of anti-skid and wear-resistant performance for asphalt pavements during the operation period. Using a combination of indoor accelerated wear tests and field detection, mixed specimens are prepared with SBS modified asphalt, limestone, and basalt aggregates. Through accelerated wear tests of different durations, the structural depth and friction coefficient are measured. Combined with the field data from the G56 K2319 section of the Hangrui Expressway, the decay laws of anti-skid performance are analyzed, and prediction models are established. The results show that the anti-skid performance of basalt mixtures is superior to that of limestone. The deepened structure technology significantly enhances the performance of basalt but has a negative impact on the pendulum value of limestone. The influence degrees of wear duration, aggregate type, and deepened structure state on structural depth and pendulum value vary. The initial structural depth of basalt mixtures (0.85 mm) is 11.8% higher than that of limestone (0.76 mm). The longitudinal pendulum value of basalt (44) is 10% higher than that of limestone (40), while the transverse pendulum value of limestone (50) is 4.2% higher than that of basalt (48). After 21 h of wear, the structural depth of basalt (0.68 mm) is 4.6% higher than that of limestone (0.65 mm), with a decay rate 23.6% lower. The pendulum value of basalt remains above 50, while limestone’s longitudinal pendulum value drops to 36 (10% lower than its initial value), even below the unmodified state. The influence order for structural depth is deepened structure state > wear duration > aggregate type, and for lateral pendulum value, it is wear duration > deepened structure state > aggregate type. There is a significant linear relationship between structural depth/pendulum value and wear duration, and the prediction models are reliable. The indoor accelerated wear of 44.5 h is equivalent to the field operation wear of 3 years. The research findings provide a theoretical basis for the evaluation of anti-skid performance, maintenance decision-making, and material optimization of asphalt pavements.
The objective of this study was to design mixtures that satisfy multiple performance criteria to build long-life pavement. A balanced mix design was employed to optimize AC-16, BBME-13, and EME-20 mixtures. The initial asphalt contents were determined using 4% air voids for the AC-16 mixture and the abundance coefficient K for BBME-13 and EME-20. Mixtures with two additional asphalt contents were also tested. A uniaxial penetration test, semi-circle bending test (to measure the flexibility index), and semi-circle bending test (to measure fracture energy) were used as performance tests. Then, a performance space diagram was created for a balanced analysis of the mixtures’ high-, intermediate-, and low-temperature performance. Finally, fatigue performance was verified. The results show that BMD could be used to evaluate different asphalt mixtures. The 20# BBME-13 (5.1%, 5.4%, and 5.7%), 50# BBME-13 5.4%, and 20# AC-16 4.7% mixtures had well-balanced performances and are recommended. The BBME-13 and EME-20 mixtures had higher fatigue lives and lower sensitivity to stress than the AC-16 mixture. For the BBME-13 and AC-16 mixtures, reducing the asphalt grade significantly increased fatigue life and decreased the sensitivity to stress. At a low stress ratio, the 20# EME-20 mixture had the best fatigue performance, whereas at a high stress ratio, the 20# BBME-13 mixture had the best fatigue performance.