Magneto-elasto-electric (ME) coupling heterostructures, consisting of piezoelectric layers bonded to magnetostrictive ones, provide for a new class of electromagnetic emitter materials on which a portable (area ~ 16 cm2) very low frequency (VLF) transmitter technology could be developed. The proposed ME transmitter functions as follows: (a) a piezoelectric layer is first driven by alternating current AC electric voltage at its electromechanical resonance (EMR) frequency, (b) subsequently, this EMR excites the magnetostrictive layers, giving rise to magnetization change, (c) in turn, the magnetization oscillations result in oscillating magnetic fields. By Maxwell’s equations, a corresponding electric field, is also generated, leading to electromagnetic field propagation. Our hybrid piezoelectric-magnetostrictive transformer can take an input electric voltage that may include modulation-signal over a carrier frequency and transmit via oscillating magnetic field or flux change. The prototype measurements reveal a magnetic dipole like near field, demonstrating its transmission capabilities. Furthermore, the developed prototype showed a 104 times higher efficiency over a small-circular loop of the same area, exhibiting its superiority over the class of traditional small antennas.
Magnetoelectric (ME) gyrators are unique circuit elements capable direct conversion of current to voltage or vice versa. In order to understand power conversion and loss processes in the gyrators, an equivalent input loss factor has been developed based on Mason's model (equivalent circuit model). This factor serves to understand the loss transferring mechanism and to evaluate the conversion efficiency for the electric power in ME gyrators. Studies have been carried out for modeling the power conversion in both the solenoid and the ME core. Several important factors have been proposed and discussed to enhance conversion efficiencies in the electric-magnetic-mechanical three-phase conversion process. A simplification of our equations reveal that the efficiency of the ME gyrator is related to the product of the effective coupling (k2eff,m) and mechanical quality (Qmech). According to our model, magnetic and electric materials with high keff,m and Qmech values are the key ingredients to enhance the efficiency of ME gyrators. We have successfully realized a power efficiency of 92% based on a Metglas/hard-PZT ME gyrator, which showed a good correlation to the predicted values.
For ( 001 ) c oriented BaTiO 3 thin films, it has been found that epitaxial constraint can result in a dramatic increase in the temperature of a tetragonal ( T ) structuralphase transition. For 2000 - Å -thick filmsgrown directly on SrTiO 3 substrates, a T → cubic ( C ) phase transition was found on heating at > 950 K , where the lattice constant changed smoothly with temperature. It was also found for films of the same thickness that the T → C transition is nearly restored to that of bulk crystals by the use of a buffer layer, which relaxes the epitaxial constraint. These results provide evidence of an epitaxially induced high temperature structuralphase transition in BaTiO 3 thin films, where the ferroelectric (internal) and structural (external) aspects of the phase transition are decoupled.
28 February 2018 in Journal of Physics: Condensed Matter
The relaxor PbMg 1/3 Nb 2/3 O 3 (PMN) has received attention due to its potential applications as a piezoelectric when doped with PbTiO 3 (PT). Previous results have found that there are two phases existing in the system, one linked to the near-surface regions of the sample, the other in the bulk. However, the exact origin of these two phases is unclear. In this paper, depth dependant analysis results from negative muon implantation experiments are presented. It is shown that the Pb content is constant throughout all depths probed in the sample, but the Mg and Nb content changes in the near-surface region below 100 μ m. At an implantation depth of 60 μ m, it is found that there is a 25% increase in Mg content, with a simultaneous 5% decrease in Nb content in order to maintain charge neutrality. These results show that the previously observed skin effects in PMN are due to a change in concentration and unit cell.