In this study, two-dimensional V2CTx MXenes were prepared by an accessible and rapid method, which involved aluminothermic combustion synthesis of the V2AlC MAX phase and its further processing in an HCl/LiF mixture under hydrothermal conditions.
Three-phase polymer composites are promising materials for creating electronic device components. The qualitative and quantitative composition of such composites has a significant effect on their functional, in particular dielectric properties. In this study, ceramic filler K2Ni0.93Ti7.07O16 (KNTO) with Ag coating as conductive additive (0.5, 1.0, 2.5 wt.%) was introduced into the polyvinylidene difluoride (PVDF) polymer matrix in amounts of 7.5, 15, 22.5, and 30 vol.%. to optimize the dielectric constant and dielectric loss tangent. The filler was characterized by X-ray phase analysis, Fourier-transform infrared spectroscopy and Scanning electron microscopy methods. The dielectric constant, dielectric loss tangent, and conductivity of three-phase composites KNTO@Ag-PVDF were studied in comparison with two-phase composites KNTO-PVDF in the frequency range from 102 Hz to 106 Hz. The dielectric constant values of composites containing 7.5, 15, 22.5, and 30 vol.% filler were 12, 13, 17.4, 19.2 for pure KNTO and 13, 19, 25, 31 for KNTO@Ag filler (2.5 wt.%) at frequency 10 kHz. The dielectric loss tangent ranged from 0.111 to 0.340 at a filler content of 7.5 to 30 vol.%. A significantly enhanced balance of dielectric properties of PVDF-based composites was found with K2Ni0.93Ti7.07O16 as ceramic filler for 1 wt.% of silver. Composites KNTO@Ag(1 wt.%)-PVDF can be applied as dielectrics for passive elements of flexible electronics.
In this study, the electrochemical energy storage properties of Ti3C2Tx MXene films have been improved by the addition of W1.33CTz MXenes with ordered vacancies in their structure.
In this paper, LixCa(1−x)Cu3Ti4O12 (LCCTO) solid solutions were successfully synthesized. XRD diagrams showed that dopant acceptor Li+ cations, in a concentration range of x = 0.01–0.10, were successfully merged into CCTO structure. It was found that doping with low concentrations of lithium (x < 0.05) inhibited grain growth during annealing; however, for x > 0.05, the grain growth process resumed. Permittivity and dielectric losses of obtained LCCTO ceramics were analyzed by the means of impedance spectroscopy in a frequency range from 10−1 to 106 Hz. It was revealed that acceptor doping with lithium at an appropriate concentration of x = 0.05 allowed to obtain ceramics with a permittivity level of ε′ = 3 × 104 and low dielectric losses tanδ < 0.1 at 1 kHz. Further addition of lithium in a concentration range of x = 0.075–0.10 led to a sharp decline in permittivity and an increase in dielectric losses. It was discovered that lithium addition to CCTO ceramics drastically decreased grain boundary resistivity from 115 MΩ·cm to 5–40 MΩ·cm at x = 0.01–0.10. Using Havriliak–Negami equation, the relaxation times for grain dipoles and grain boundary dipoles were found to be ranging from 0.8 × 10−6 to 1.7 × 10−6 s and from 0.4 × 10−4 to 7.1 × 10−4 s, respectively. The developed materials can be used in the manufacture of Multilayer Ceramic Capacitors (MLCC) as a dielectric.
Some solid solutions with the chemical composition KxFeyTi8-yO16 (KFTO) and a hollandite-like structure were successfully synthesized by modified sol–gel method. The obtained powders were characterized using X-ray diffraction (XRD) and scanning electron microscopy (SEM). The ceramic pellets based on KFTO powders were obtained by compressing and sintering at 1080 °C for 4 h. The sinters were characterized by X-ray and impedance spectroscopy. XRD results show that KFTO powders have a mono-phase tetragonal structure at x = 1.4–1.8 and y = 1.4–1.6. However, it was recognized that the hollandite-like phase could be broken during sintering to form TiO2 and Fe2TiO5 crystals distributed throughout the volume of the ceramics. A frequency dependency of dielectric properties for the sinters was studied by impedance spectroscopy. It was found that an increase in the TiO2 (rutile) phase during the sintering contributes to a decrease in dielectric losses. At the same time, the KFTO ceramics with reduced content of potassium had increased permittivity. The contribution of electron-pinned defect dipoles (EPDD) and internal barrier layer capacitance (IBLC) in the permittivity of the obtained ceramics was estimated using the Havriliak–Negami equation. It is shown that the KFTO ceramics have the polydisperse characteristic of dielectric relaxation. The observed grain and grain boundary dipole relaxation times were 1.03 × 10−6 to 5.51 × 10−6 s and 0.197 to 0.687 s, respectively.