Probing polycrystals' stress: The way that a polycrystalline material deforms is in part determined by internal stresses between and within crystal grains. Hayashi et al. developed an x-ray method for mapping the intragranular stresses in a polycrystalline material. They found surprisingly large stresses, which are important for the fundamental understanding of how these materials will fail. This method will work for other materials and provides important information for multiscale deformation modeling. Science , this issue p. 1492
Recently, nondestructive evaluation of the stresses localized in grains was achieved for plastically deformed low-carbon steel using scanning three-dimensional X-ray diffraction (S3DXRD) microscopy with a conical slit. However, applicable metals and alloys were restricted to a single phase and evaluated stress was underestimated due to the fixed Bragg angles of the conical slit optimized to αFe. We herein propose S3DXRD with a rotating spiral slit adaptable to various metals and alloys and accurate stress evaluation with sweeping Bragg angles. Validation experiments with a 50-keV X-ray microbeam were conducted for low-carbon steel as a body-centered cubic (BCC) phase and pure Cu as a face-centered cubic (FCC) phase. As a result of orientation mapping, polygonal grain shapes and clear grain boundaries were observed for both BCC and FCC metals. Thus, it was demonstrated that S3DXRD with a rotating spiral slit will be applicable to various metals and alloys, multiphase alloys, and accurate stress evaluation using a X-ray microbeam with a higher photon energy within an energy range determined by X-ray focusing optics. In principle, this implies that S3DXRD becomes applicable to larger and thicker metal and alloy samples instead of current miniature test or wire-shaped samples if a higher-energy X-ray microbeam is available.
25 August 2023 in Journal of Applied Crystallography
The spatial resolution in scanning-based two-dimensional microscopy is normally limited by the size of the probe, thereby a smaller probe is a prerequisite for enhancing the spatial resolution. For three-dimensional microscopy that combines translation and rotation motions of a specimen, however, complex trajectories of the probe highly overlap in the specimen, which could change the postulate above. Here, the spatial resolution achieved in scanning three-dimensional X-ray diffraction (s3DXRD) microscopy is investigated. In this method, the most appropriate orientation of the pixel in the specimen coordinate is selected by comparing the completeness of diffraction peaks with theory. Therefore, the superposed area of the beam trajectory has a strong effect on the spatial resolution, in terms of the completeness of diffraction peaks. It was found that the highly superposed area by the incident X-rays, which has the highest completeness factor in the pixel of the specimen, is much smaller than the X-ray probe size, and that sub-pixel analysis by dividing a pixel into small pieces leads to drastic improvement of the spatial resolution in s3DXRD.
Plastically deformed low-carbon steel has been analyzed by nondestructive three-dimensional orientation and strain mapping using scanning three-dimensional X-ray diffraction microscopy (S3DXRD). However, the application of S3DXRD is limited to single-phase alloys. In this study, we propose a modified S3DXRD analysis for dual-phase alloys, such as ferrite–pearlite carbon steel, which is composed of grains detectable as diffraction spots and a phase undetectable as diffraction spots. We performed validation experiments for ferrite–pearlite carbon steel with different pearlite fractions, in which the ferrite grains and the pearlite corresponded to the detectable grains and an undetectable phase, respectively. The regions of pearlite appeared more remarkably in orientation maps of the ferrite grains obtained from the carbon steel samples than that of the single-phase low-carbon steel and increased with the increase in the carbon concentration. The fractions of the detectable grains and the undetectable phase were determined with an uncertainty of 15%–20%. These results indicate that the proposed modified analysis is qualitatively valid for dual-phase alloys comprising detectable grains and an undetectable phase.