Magnetic sensors are key elements in many industrial, security, military, and biomedical applications. Heusler alloys are promising materials for magnetic sensor applications due to their high spin polarization and tunable magnetic properties. The dynamic field range of magnetic sensors is strongly related to the perpendicular magnetic anisotropy (PMA). By tuning the PMA, it is possible to modify the sensing direction, sensitivity and even the accuracy of the magnetic sensors. Here, we report the tuning of PMA in a Co2MnGa Heusler alloy film via argon (Ar) ion irradiation. MgO/Co2MnGa/Pd films with an initial PMA were irradiated with 30 keV 40Ar+ ions with fluences (ions·cm−2) between 1 × 1013 and 1 × 1015 Ar·cm−2, which corresponds to displacement per atom values between 0.17 and 17, estimated from Monte-Carlo-based simulations. The magneto optical and magnetization results showed that the effective anisotropy energy (Keff) decreased from ~153 kJ·m−3 for the un-irradiated film to ~14 kJ·m−3 for the 1 × 1014 Ar·cm−2 irradiated film. The reduced Keff and PMA are attributed to ion-irradiation-induced interface intermixing that decreased the interfacial anisotropy. These results demonstrate that ion irradiation is a promising technique for shaping the PMA of Co2MnGa Heusler alloy for magnetic sensor applications.
A low voltage (−20 V) operating high-energy (5.48 MeV) α-particle detector with a high charge collection efficiency (CCE) of approximately 65% was observed from the compensated (7.7 × 1014 /cm3) metalorganic vapor phase epitaxy (MOVPE) grown 15 µm thick drift layer gallium nitride (GaN) Schottky diodes on free-standing n+-GaN substrate. The observed CCE was 30% higher than the bulk GaN (400 µm)-based Schottky barrier diodes (SBD) at −20 V. This is the first report of α–particle detection at 5.48 MeV with a high CCE at −20 V operation. In addition, the detectors also exhibited a three-times smaller variation in CCE (0.12 %/V) with a change in bias conditions from −120 V to −20 V. The dramatic reduction in CCE variation with voltage and improved CCE was a result of the reduced charge carrier density (CCD) due to the compensation by Mg in the grown drift layer (DL), which resulted in the increased depletion width (DW) of the fabricated GaN SBDs. The SBDs also reached a CCE of approximately 96.7% at −300 V.
Diamond-like carbon (DLC) coatings were deposited with a new direct ion deposition system using a novel 360 degree ion source operating at acceleration voltage between 4 and 8 kV. Cross-sectional TEM images show that the coatings have a three layered structure which originates from changes in the deposition parameters taking into account ion source condition, ion current density, deposition angles, ion sputtering and ion source movement. Varying structural growth conditions can be achieved by tailoring the deposition parameters. The coatings show good promise for industrial use due to their high hardness, low friction and excellent adhesion to the surface of the samples.